Sandvik 29.9

Welding wire Datasheet

Datasheet updated 2017-09-19 16:25 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 29.9 is a filler material suitable for joining dissimilar steels and for overlay welding of carbon and low-alloy steels. It gives a ferritic-austenitic structure with a high ferrite content.

Standards

  • ISO 14343: 29 9
  • AWS A5.9/ASME SFA-5.9: ER312
  • W.Nr.: 1.4337

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.