Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 53 is a nickel-chrome-cobalt-molybdenum alloy of type alloy 617. It has an excellent resistance to high temperature corrosion such as oxidation and carburization. The weld metal provides a combination of excellent metallurgical stability and strength in short and long term exposure to temperatures up to 1100°C (2012°F).

Applications for Sanicro® 53 are found in high temperature heat exchangers and valves, furnace tubing in the petrochemical industry, radiant heat tubes, gas turbines, components subjected to high temperatures in the chemical processing industry and components for power plants.

Sanicro® 53 is suitable for joining heat resistant nickel alloys, heat resistant austenitic and cast alloys such as:

  • UNS N08810 (1.4958)
  • UNS N08811 (1.4959)
  • UNS N06617 (2.4663)

Sanicro 53 can also be used for surfacing.

Standards

  • ISO 18274: NiCr22Co12Mo9/Ni 6617
  • AWS A5.14/ASME A5.14: ERNiCrCoMo-1
  • W.Nr.: 2.4663

Product Approvals

  • CE

Contact your nearest sales office for details.

Please note that the Werkstoff Nr. corresponds to the base material of the same grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.