Sanicro® 59

Welding wire Datasheet

Datasheet updated 2018-07-30 07:08 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 59 is a nickel-chrome-molybdenum alloy of type alloy 59. It is a versatile alloy with excellent wet corrosion resistance for the most demanding applications. It combines excellent corrosion resistance in oxidizing and reducing media, has excellent resistance in chloride containing media and to localized corrosion environments. Sanicro® 59 has excellent thermal stability compared to other common nickel alloys and has therefore outstanding resistance to intermetallic precipitation during welding. Applications for Sanicro® 59 are found in aggressive and contaminated corrosive media including scrubbers for flue gas desulfurization (FGD), chemical process plants and in severe offshore and petrochemical environments.

Sanicro® 59 is used for joining matching alloys or dissimilar joining to other nickel alloys such as UNS N10276 (2.4819), type UNS N06022 (2.4602), UNS N06625 (2.4856) and N08825 (2.4858). It provides strong, tough, Nb-free weld metal for dissimilar welds in super-austenitic and super-duplex stainless steel joints or combinations of these with nickel alloys. Sanicro® 59 can be used for surfacing.

Standards

  • ISO 18274: NiCr23Mo16/Ni 6059
  • AWS A5.14/ASME SFA-5.14: ERNiCrMo-13
  • W.Nr.: 2.4605

Product Approvals

  • ISO 15156/NACE MR0175
  • CE
  • TÜV

Contact your nearest sales office for details.

Please note that the Werkstoff Nr. corresponds to the base material of the same grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.