Sanicro® 60

Welding wire Datasheet

Datasheet updated 2019-07-12 13:10 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 60 welding wire is suitable for joining nickel-chromium-molybdenum nickel alloys and chromium-nickel-molybdenum steels with very high corrosion resistance in oxidizing, aqueous and high temperature environments such as 6Mo-steels, UNS N06625 (2.4856) and corresponding grades. It is also suitable for joining stainless steels and nickel alloys for high-temperature service.

Sanicro® 60 can also be used for dissimilar joining of stainless steels to nickel alloys, for overlay welding and is available as both wire and rod.

Standards

  • ISO 18274: NiCr22Mo9Nb/Ni 6625
  • AWS A5.14/ASME SFA-5.14: ERNiCrMo-3
  • W.Nr.: 2.4856

Product Approvals

  • CE
  • TÜV
  • BV

Contact your nearest sales office for details.

Please note that the Werkstoff Nr. corresponds to the base material of the same grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.