Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 68HP is a filler material for welding Sanicro® 69, i.e. alloy 690, and similar alloys. It produces corrosion resistant overlays on most low-alloy and stainless steels. Sanicro® 68HP can also be used for dissimilar joints between the common nickel alloys and carbon, low-alloy and stainless steels. Sanicro® 68HP is available as wire and rods.

Standards

  • ISO 18274: NiCr30Fe9/Ni 6052
  • AWS A5.14/ASME SFA-5.14: ERNiCrFe-7

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.