Sanicro® 72HP

Welding wire Datasheet

Datasheet updated 2019-07-12 13:04 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 72HP is filler material for joining NiCrFe alloys, 9% Ni steels used at cryogenic temperatures, stainless steels to carbon steels, high service temperature NiCu alloys to carbon steels and NiCu alloys to nickel alloys. Sanicro® 72HP can be used in air up to 1175°C (2145°F) and in sulphur dioxide atmospheres up to 800°C (1470°F).

Sanicro® 72HP is suitable for MIG, TIG, PAW and SAW and available as wire and rods.

Standards

  • ISO 18274: NiCr20Mn3Nb / Ni 6082
  • AWS A5.14/ASME SFA-5.14:  ERNiCr-3

Product Approvals

  • CE
  • TÜV

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.