Exera® 11R51 / 11R51 HV medical wire

WireDatasheet

Datasheet updated 2021-11-10 06:56 (supersedes all previous editions)

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Exera® 11R51 and Exera® 11R51 HV (vacuum remelted) are austenitic stainless steels alloyed with molybdenum that are characterized by high tensile strength and high resistance to corrosion, fatigue and relaxation.

Vacuum-remelted Exera® 11R51 HV offers higher cleanliness compared to Exera® 11R51, which is usually required for medical applications.

Compared with the standard grade Exera® 12R10 medical wire, Exera® 11R51 and Exera® 11R51 HV offer:

  • Higher tensile strength and tempering effect
  • Higher relaxation resistance, especially at elevated temperatures
  • Higher fatigue strength
  • Better corrosion resistance, through the addition of molybdenum

Service temperature: -200 to 300°C (-330 to 570°F)
These grades are used for applications such as root canal files, reamers, broaches, surgical suture needles, braces, and acupuncture needles.

Standards

  • UNS: S30151
  • ISO: X9 CrNi 18-8
  • EN Number: 1.4310
  • EN Name: X10CrNi18-8

Product standards

EN 10270-3
ISO 6931-1
ASTM F 899, A 313/A 313M

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.