Exera® 12R10 / 12R10 HV medical wire

WireDatasheet

Datasheet updated 2021-02-02 14:37 (supersedes all previous editions)

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Exera® 12R10 and Exera® 12R10 HV (vacuum remelted) are austenitic stainless steels characterized by moderate tensile strength, good corrosion resistance and moderate fatigue and relaxation resistance.

Vacuum-remelted Exera® 12R10 HV offers higher cleanliness compared to Exera® 12R10, which is usually required for medical applications.

Service temperature: -200 to 250°C (-330 to 480°F).

Exera® 12R10 and Exera® 12R10 HV are characterized by:

  • High tensile strength and tempering effect
  • Good relaxation resistance, especially at elevated temperatures
  • High fatigue strength

Standards

  • ASTM: 302/302VM, '304V'
  • ISO: X9 CrNi 18-8 Grade 1 NS
  • EN Number: 1.4310 NS
  • EN Name: X10CrNi18-8NS
  • W.Nr.: 1.4310
  • JIS: SUS 302/304-WPB

Product standards

EN 10270-3
ISO 6931-1
ASTM A 313/A 313M, F899
JIS G 4314

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.