Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Exera® 5R62 and Exera® 3R65 are austenitic stainless steels alloyed with molybdenum. Exera® 3R65 is a low carbon version of Exera® 5R62.

The grades are characterized by:

  • Good resistance to general corrosion and better resistance to pitting than ASTM 304, because of the alloying with Mo
  • High tensile strength

Standards

  • ASTM: 316/316L
  • UNS: S31600/ S31603
  • ISO: 316/316L
  • EN Number: 1.4401/1.4404
  • EN Name: X5CrNiMo17-12-2/X2CrNiMo17-12-2
  • W.Nr.: 1.4401/1.4404
  • JIS: SUS316/SUS316L

Product Standards

  • ASTM F899
  • ISO 16061

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.