Exera® 7C27 medical wire

WireDatasheet

Datasheet updated 2021-02-02 16:31 (supersedes all previous editions)

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Exera® 7C27 is a martensitic stainless chromium steel characterized by very good hardening properties and very good cold formability. After hardening and tempering, the grade has very good corrosion resistance and toughness.

Exera® 7C27 is characterized by:

  • Soft delivery condition
  • Very good hardening properties
  • Very good cold formability
  • High corrosion resistance after hardening and tempering

Standards

  • ASTM: 420
  • AWS: ER 420
  • EN Number: 1.4028 Mod./1.4031 Mod.
  • W.Nr.: 1.4007
  • DIN: X35Cr14
  • SS: 2304
  • AFNOR: Z 30C13(13H)

Product standards

  • ASTM F899
  • ISO 16061

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.