Exera® SAF 2205™ medical wire

WireDatasheet

Datasheet updated 2021-09-23 06:18 (supersedes all previous editions)

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Exera®SAF 2205™ is a duplex stainless steel (austenitic-ferritic) characterized by:

  • Very good fatigue resistance
  • High resistance to stress corrosion cracking in chloride-bearing environments
  • High resistance to general corrosion, pitting, and crevice corrosion
  • High resistance to erosion corrosion and corrosion fatigue
  • Physical properties that offer design advantages

Service temperature: -100 to 300°C (-150 to 570°F)

Standards

  • UNS: S32205/S31803
  • EN Number: 1.4462
  • EN Name: X2CrNiMoN22-5-3
  • W.Nr.: 1.4462

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.