Exera® SAF 2205™ SH medical wire

WireDatasheet

Datasheet updated 2021-09-23 06:19 (supersedes all previous editions)

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Exera® SAF 2205™ SH is a duplex (austenitic/ferritic) stainless steel with super high tensile strength.

The grade is characterized by:

  • Very good corrosion resistance
  • High resistance to stress corrosion cracking in chloride-bearing environments
  • High resistance to stress corrosion cracking in environments containing hydrogen sulphide
  • High resistance to general corrosion, pitting, and crevice corrosion
  • High resistance to erosion corrosion and corrosion fatigue
  • Extremely high tensile strength in 'as delivered' condition
  • Very good relaxation resistance
  • Physical properties that offer design advantages

Service temperature: -100 to 300°C (-150 to 570°F)
Service temperature: -200 to 280°C (-330 to 540°F)

Standards

  • UNS: S32205/S31803
  • EN Number: 1.4462
  • EN Name: X2CrNiMoN22-5-3
  • W.Nr.: 1.4462

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.