Sandvik 11RM20 spring wire

Wire Datasheet

Datasheet updated 2017-01-19 12:34 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 11RM20 is an austenitic stainless alloyed with manganese that is characterized by very high wear resistance. The grade is normally delivered in flat-rolled, annealed condition. Sandvik 11RM20 is primarily used for expander rings in automotive engines.

Standards

  • ASTM: 201
  • UNS: S2010075
  • EN Number: 1.4372
  • EN Name: X12CrMnNiN17-7-5
  • W.Nr.: 1.4372
  • DIN: X12CrMnNiN 17-7-5
  • JIS: SUS 201

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.