Sandvik 5R10/2R25 medical wire

Wire Datasheet

Datasheet updated 2017-01-19 12:33 (supersedes all previous editions)

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Sandvik 5R10 and Sandvik 2R25 are austenitic chromium-nickel stainless steels. Sandvik 2R25 is a low carbon version of Sandvik 5R10. The grades are characterized by:

  • Good corrosion resistance
  • Excellent toughness
  • Good welding characteristics

Standards

  • ASTM: 304, 304L
  • UNS: S30400, S30403
  • EN Number: 1.4301, 1.4306
  • EN Name: X5CrNi18-10, X2CrNi19-11
  • W.Nr.: 1.4301, 1.4306
  • DIN: X5 CrNi 18 10, X2 CrNi 19 11
  • SS: 2332, 2352
  • AFNOR: Z6 CN 18 09, Z3 CN 18 10
  • BS: 304S31

Product standards

  • ASTM F899
  • ISO 16061

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.