Sandvik NiMn2ROE

Wire Datasheet

Datasheet updated 2017-01-19 12:34 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik NiMu2ROE is a vacuum remelted nickel alloy with good characteristics for cold working fabrication and thermal demands. The grade does not permit evolution of gases during its utilization. Sandvik NiMu2ROE is typically used for lamp bulb conducting electrodes.

Standards

  • W.Nr.: 2.4110
  • DIN: 17741

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.