Sandvik SanRig 80™

Wire Datasheet

Datasheet updated 2018-07-05 14:41 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik SanRig 80™ is an austenitic stainless steel characterized by very high fatigue and tensile strength, combined with good corrosion resistance in seawater containing media. Sandvik SanRig 80™ rig rod is developed specially for marine applications.

Standards

  • UNS: S31675

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.