SANICRO 35: Exploring Refinery applications and results from laboratory testing

During this webinar, we will discuss the general mechanical and corrosion properties of Sanicro® 35, a new high alloyed, super-austenitic grade developed by Sandvik Materials Technology. The recently launched grade is seen as a cost-effective alternative to nickel-base alloys for most industries. We will also discuss the suitability of the grade for specific refinery applications such as REAC.