Round bar sizes and grades

The standard range of round bar includes several grades of nickel alloys
and stainless steel. Other grades can be offered on request.
Round bars are delivered in random or cut to fixed lengths.
Grade | UNS | ASTM | EN | C | Cr | Ni | Mo | Nb | Others |
---|---|---|---|---|---|---|---|---|---|
Sanicro® 625 | N06625 | UNS N06625 Grade 1 | 2.4856 | 0.025 | 21 | 62 | 8.5 | 3.5 | - |
Sanicro® 825 | N08825 | UNS N08825 | 2.4858 | ≤0.030 | 22.5 | 40.5 | 3.4 | - | - |
Sanmac® 22051) | S31803/32205 | - | 1.4462 | ≤0.030 | 22.5 | 5.5 | 3.2 | N | |
SAF 2205™+ | S31803/32205 | - | 1.4462 | ≤0.030 | 22.5 | 5.5 | 3.2 | N | |
SAF 32760™ | S32760 | - | 1.4501 | ≤0.030 | 25 | 7 | 3.8 | W, Cu, N | |
SAF 2507®1) | S32750 | - | 1.4410 | ≤0.030 | 25 | 7 | 4 | N | |
Sanmac® 329 | S32900 | - | 1.4460 | ≤0.05 | 25.5 | 5 | 1.5 | N | |
Sanicro® 28 | N08028 | - | 1.4563 | ≤0.020 | 27 | 31 | 3.5 | Cu | |
Sanmac® 304/304L | S30400/S30403 | 304/304L | 1.4301/1.4307 | ≤0.030 | 18.5 | 8.5 | - | - | |
Sanmac® 316/316L1) | S31600/S31603 | 316/316L | 1.4401/1.4404 | ≤0.030 | 17 | 10.5 | 2.1 | - | |
Sanmac® 4435 | S31600/S31603 | 316/316L | 1.4435 | ≤0.030 | 17.5 | 12.5 | 2.6 | - | |
Sanmac® 4571 | S31635 | 316Ti | 1.4571 | 0.03 | 17 | 11 | 2.1 | Ti |
Nickel alloy bars
Nickel alloy bar standards
Nickel based bar steel - stock and production orders | |||||||
---|---|---|---|---|---|---|---|
Grade | ASTM B425 | ASME SB425 | ASTM B446 | ASME SB446 | NACE MR0175 / ISO15156 | NACE MR0103 / ISO17945 | PED 2014/68/EU |
Sanicro®625 | - | - | 75-230 mm 2.95-9.05" | 75-230 mm 2.95-9.05" | Independent of size | Independent of size | - |
Sanicro®825 | 20-250 mm 0.79-9.84" | 20-250 mm 0.79-9.84" | - | - | Independent of size | Independent of size | Independent of size |
Nickel alloy bar product range
Random length 3-6.9 m (9.8-22.6 ft) | |||||||
---|---|---|---|---|---|---|---|
Sanicro 625 stock assortment | |||||||
Diameter | Tolerance | Random length | Weight | ||||
mm | inch | mm | inch | m | ft | kg/m | lb/ft |
76.2 | 3.0 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 38 | 25.7 |
88.9 | 3.5 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 52 | 35.0 |
101.6 | 4.0 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 68 | 45.6 |
114.3 | 4.5 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 86 | 57.7 |
127 | 5.0 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 106 | 71.2 |
139.7 | 5.5 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 128 | 86.1 |
152.4 | 6.0 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 152 | 102.4 |
165.1 | 6.5 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 179 | 120.1 |
177.8 | 7.0 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 207 | 139.3 |
190.5 | 7.5 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 238 | 159.8 |
203.2 | 8.0 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 271 | 181.8 |
215.9 | 8.5 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 305 | 205.2 |
228.6 | 9.0 | 0/+0.79 | 0/+0.031 | 3-6.9 | 9.8-22.6 | 342 | 230.0 |
Sanicro 625 production orders | |||||||
Diameter | |||||||
From | To | Tolerance | |||||
mm | inch | mm | inch | mm | inch | ||
75 | 2.95 | 230 | 9.05 | 0/+0.79 | 0/+0.031 |
Stainless Steel Bars
Grade | IOGP S-536 ISO 17781 |
NORSOK M630 ed.6 | EN 10088-3 | EN 10272 | AD2000- W2/W10 |
ASTM A 479 | ASME SA 479 | NACE MR 0175 |
---|---|---|---|---|---|---|---|---|
Sanmac® 316/316L | 20-450 mm | 20-450 mm | 20-450 mm | 20-250 mm | 20-375 mm |
20-450 mm | 20-450 mm | Independent of size |
Sanmac® 2205 | - | 20-260 mm | 20-450 mm | 20-160 mm | - | 20-450 mm | 20-450 mm | Independent of size |
SAF 2205™+ | 20-260 mm | 20-260 mm | 20-450 mm | 20-160 mm | - | 20-450 mm | 20-450 mm | Independent of size |
SAF 32760™ | - | 80-180 mm | 80-180 mm | 20-160 mm | - | 20-450 mm | 20-450 mm | Independent of size |
SAF 2507® | 20-250 mm | 20-160 mm | - | 20-250 mm | 20-250 mm | Independent of size |
* Please contact us for information about standards for grades not included in the table.
Diameter, mm (in.) |
Tolerance, mm (in.) |
Random length, m (ft) |
Weight kg/m (lb/ft) |
Sanmac 316L |
Sanmac 329 |
Sanmac 2205 |
Sandvik SAF 32760 |
Sandvik SAF 2507 |
---|---|---|---|---|---|---|---|---|
20.00 (0.79) | -0/+0.13 (-0/+0.005) | 3.5–4.5 (11.5-14.8) | 2.5 (1.7) | □ | □ | ■ | □ | ■ |
25.00 (0.98) | -0/+0.13 (-0/+0.005) | 3.5–4.5 (11.5-14.8) | 3.9 (2.6) | □ | □ | ■ | □ | ■ |
30.00 (1.18) | -0/+0.13 (-0/+0.005) | 3.5–4.5 (11.5-14.8) | 5.5 (3.7) | ■ | □ | ■ | □ | ■ |
35.00 (1.38) | -0/+0.16 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 7.6 (5.1) | □ | □ | ■ | □ | ■ |
40.00 1.57) | -0/+0.16 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 9.9 (6.7) | ■ | □ | ■ | □ | ■ |
45.00 (1.77) | -0/+0.16 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 12.5 (8.4) | □ | □ | ■ | □ | ■ |
50.00 (1.97) | -0/+0.16 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 15.4 (10.3) | ■ | □ | ■ | □ | ■ |
52.00 (2.04) | -0/+0.16 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 17.3 (11.6) | - | ■ | - | - | - |
55.00 (2.16) | -0/+0.19 (-0/+0.007) | 3.5–4.5 (11.5-14.8) | 19.0 (12.8) | □ | □ | ■ | □ | ■ |
60.00 (2.36) | -0/+0.19 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 22.2 (14.9) | ■ | □ | ■ | □ | ■ |
61.20 (2.41) | -0/+0.19 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 22.6 (15.2) | - | ■ | - | - | - |
65.00 (2.56) | -0/+0.19 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 26.0 (17.5) | □ | □ | ■ | □ | ■ |
66.20 (2.60) | -0/+0.19 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 27.1 (18.2) | □ | ■ | □ | □ | □ |
70.00 (2.76) | -0/+0.19 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 30.2 (20.3) | ■ | □ | ■ | □ | ■ |
71.40 (2.81) | -0/+0.19 (-0/+0.006) | 3.5–4.5 (11.5-14.8) | 30.8 (20.7) | - | ■ | - | - | - |
75.00 (2.95) | -0/+1.00 (-0/+0.039) | 5–7 (16.4-23.0) | 34.7 (23.3) | ■ | □ | ■ | □ | ■ |
76.40 (3.00) | -0/+1.00 (-0/+0.039) | 5-7 (16.4-23.0) | 36 (24.2) | □ | ■ | □ | □ | □ |
80.00 (3.15) | -0/+1.00 (-0/+0.039) | 5–7 (16.4-23.0) | 39.5 (26.6) | ■ | □ | ■ | ■ | ■ |
81.40 (3.20) | -0/+1.00 (-0/+0.039) | 5–7 (16.4-23.0) | 40.2 (27.0) | - | ■ | - | - | - |
82.55 (3.25) | -0/+1.00 (-0/+0.039) | 5-7 (16.4-23.0) | 41.9 (28.1) | □ | □ | □ | ■ | □ |
85.00 (3.35) | -0/+1.00 (-0/+0.039) | 5–6.9 (16.4-22.6) | 44.6 (30.0) | ■ | □ | ■ | □ | ■ |
86.40 (3.40) | -0/+1.00 (-0/+0.039) | 5–6.9 (16.4-22.6) | 45.3 (30.4) | - | ■ | - | - | |
88.00 (3.46) | -0/+1.00 (-0/+0.039) | 5-7 (16.4-23.0) | 47.7 (32.0) | □ | ■ | □ | □ | □ |
90.00 (3.54) | -0/+1.00 (-0/+0.039) | 5–7 (16.4-23.0) | 49.9 (33.5) | ■ | □ | ■ | ■ | ■ |
95.00 (3.74) | -0/+1.00 (-0/+0.039) | 3–7 (16.4-23.0) | 55.6 (37.4) | ■ | □ | ■ | □ | ■ |
96.40 (3.80) | -0/+1.00 (-0/+0.039) | 5-7 (16.4-23.0) | 57.2 (38.4) | □ | ■ | □ | □ | □ |
98.00 (3.86) | -0/+1.00 (-0/+0.039) | 5-7 (16.4-23.0) | 59.2 (39.8) | □ | ■ | □ | □ | □ |
100 (3.94) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 61.7 (41.5) | ■ | □ | ■ | □ | ■ |
101.60 (4.00) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 63.6 (42.7) | □ | □ | □ | ■ | □ |
102 (4.02) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 63.9 (43.0) | - | ■ | - | - | - |
105 (4.13) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 68.0 (45.7) | ■ | □ | ■ | □ | ■ |
107 (4.21) | -0/+1.50 (-0/+0.059) | 5-7 (16.4-23.0) | 70.6 (47.4) | □ | ■ | □ | □ | □ |
110 (4.33) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 74.6 (50.0) | ■ | □ | ■ | □ | ■ |
112 (4.41) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 75.9 (51.0) | - | ■ | - | - | - |
114.3 (4.50) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 80.5 (54.1) | □ | □ | □ | ■ | □ |
115 (4.53) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 81.5 (54.8) | ■ | ■ | ■ | □ | ■ |
117 (4.61) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 82.9 (55.7) | - | ■ | - | - | - |
120 (4.72) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 88.8 (59.8) | ■ | □ | ■ | □ | ■ |
120.65 (4.75) | -0/+1.50 (-0/+0.059) | 5-7 (16.4-23.0) | 89.7 (60.3) | □ | □ | □ | ■ | □ |
122 (4.80) | -0/+1.50 (-0/+0.059) | 5-7 (16.4-23.0) | 91.8 (61.7) | □ | ■ | □ | □ | □ |
125 (4.92) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 96.3 (64.7) | ■ | □ | ■ | □ | ■ |
127 (5.00) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 99.4 (66.8) | □ | □ | □ | ■ | □ |
130 (5.12) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 104 (69.9) | ■ | □ | ■ | ■ | ■ |
132 (5.20) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 107 (71.7) | □ | ■ | □ | □ | □ |
133.35 (5.25) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 110 (73.9) | □ | □ | ■ | □ | ■ |
135 (5.31) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 112 (75.3) | ■ | □ | ■ | □ | ■ |
140 (5.51) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 121 (81.3) | ■ | □ | ■ | ■ | ■ |
143 (5.63) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 126 (84.7) | □ | ■ | □ | □ | □ |
145 (5.71) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 130 (87.4) | ■ | □ | ■ | □ | ■ |
150 (5.90) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 139 (93.4) | ■ | □ | ■ | ■ | ■ |
152.4 (6.00) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 143 (96.1) | □ | □ | □ | ■ | □ |
153 (6.02) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 144 (96.8) | □ | ■ | □ | □ | □ |
155 (6.10) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 149 (100.1) | ■ | □ | ■ | □ | ■ |
160 (6.30) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 158 (106.2) | ■ | □ | ■ | ■ | ■ |
163 (6.42) | -0/+1.50 (-0/+0.059) | 5–7 (16.4-23.0) | 164 (110.2) | □ | ■ | □ | □ | □ |
165 (6.50) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 168 (112.9) | ■ | □ | ■ | □ | ■ |
165.1 (6.50) | -0/+1.50 (-0/+0.059) | 5-6 (16.4-19.7) | 168 (112.9) | □ | □ | □ | ■ | □ |
170 (6.69) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 178 (119.6) | ■ | □ | ■ | ■ | ■ |
173 (6.81) | -0/+1.50 (-0/+0.059) | 5-6 (16.4-19.7) | 185 (124.3) | □ | ■ | □ | □ | □ |
175 (6.89) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 189 (127.0) | ■ | □ | ■ | □ | ■ |
180 (7.09) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 200 (134.4) | ■ | □ | ■ | ■ | ■ |
184 (7.24) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 209 (140.4) | - | ■ | - | - | - |
185 (7.28) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 211 (141.8) | ■ | □ | ■ | - | ■ |
190 (7.48) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 223 (149.8) | ■ | □ | ■ | - | ■ |
200 (7.87) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 247 (166.0) | ■ | □ | ■ | - | ■ |
203.2 (8.00) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 255 (171.3) | ■ | □ | □ | - | □ |
205 (8.07) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 260 (174.7) | ■ | □ | ■ | - | ■ |
210 (8.27) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 272 (182.8) | ■ | □ | ■ | - | ■ |
220 (8.66) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 298 (200.2) | ■ | □ | ■ | - | ■ |
225 (8.96) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 312 (209.6) | ■ | □ | ■ | - | ■ |
230 (9.05) | -0/+1.50 (-0/+0.059) | 5–6 (16.4-19.7) | 326 (219.1) | ■ | □ | ■ | - | ■ |
240 (9.45) | -0/+1.50 (-0/+0.059) | 3–6.2 (9.8-20.3) | 355 (238.5) | ■ | □ | ■ | - | ■ |
250 (9.84) | -0/+1.50 (-0/+0.059) | 3–5.9 (9.84-19.3) | 385 (258.7) | ■ | □ | ■ | - | ■ |
254 (10.00) | -0/+1.50 (-0/+0.059) | 3–5.7 (9.84-25.9) | 398 (267.4) | ■ | □ | □ | - | □ |
260 (10.24) | -0/+1.50 (-0/+0.059) | 3–6.9 (9.84-22.6) | 417 (280.2) | ■ | □ | ■ | - | □ |
270 (10.63) | -0/+1.50 (-0/+0.059) | 3–5 (9.84-16.4) | 450 (302.4) | ■ | □ | ■ | - | □ |
280 (11.00) | -0/+1.50 (-0/+0.059) | 3–7 (9.84-25.9) | 483 (324.6) | ■ | □ | ■ | - | □ |
285 (11.22) | -0/+1.50 (-0/+0.059) | 3–5 (9.84-16.4) | 501 (336.7) | ■ | □ | ■ | - | □ |
300 (11.81) | -0/+2.00 (-0/+0.079) | 3–5 (9.84-16.4) | 555 (372.9) | ■ | □ | ■ | - | □ |
320 (12.60) | -0/+2.00 (-0/+0.079) | 3–5 (9.84-16.4) | 631 (424.0) | ■ | □ | ■ | - | - |
325 (12.80) | -0/+2.00 (-0/+0.079) | 3–5 (9.84-16.4) | 651 (437.4) | ■ | □ | ■ | - | - |
340 (13.39) | -0/+2.00 (-0/+0.079) | 3–5 (9.84-16.4) | 713 (479.1) | ■ | □ | ■ | - | - |
350 (13.78) | -0/+2.00 (-0/+0.079) | 3–5 (9.84-16.4) | 755 (507.3) | ■ | □ | ■ | - | - |
375 (14.76) | -0/+3.00 (-0/+0.12) | 3–5 (9.84-16.4) | 867 (582.6) | ■ | □ | ■ | - | - |
400 (15.75) | -0/+3.00 (-0/+0.12) | 3–5 (9.84-16.4) | 987 (663.2) | ■ | □ | ■ | - | - |
406.4 (16.00) | -0/+3.00 (-0/+0.12) | 3–5 (9.84-16.4) | 1043 (701.0) | ■ | □ | □ | - | - |
425 (16.73) | -0/+3.00 (-0/+0.12) | 3–5 (9.84-16.4) | 1114 (748.6) | ■ | □ | ■ | - | - |
450 (17.72) | -0/+3.00 (-0/+0.12) | 3–5 (9.84-16.4) | 1249 (839.3) | ■ | □ | ■ | - | - |