Standard sizes in metric units (other sizes can be offered on request)
Denomination Nominal
bar size
mm
tolerance
mm
Hole dia.
incl. ovality
mm
Eccentricity1)
max
mm
Random2)
length
m (±10%)
Weight
kg/m
H 19 19.03 ±0.18 6.0±0.4 0.55 5- 6 2.23
H 22 22.20 +0.20/-0.15 6.7±0.4 0.6 7.5- 8.5 3.06
H 22 22.05 +0.20/-0.15 7.25±0.5 0.6 7.5- 8.5 2.94
H 25 25.35 +0.20/-0.23 7.6±0.5 0.7 5.5- 6.5 4.00