Sizes and tolerances for Sanbar® 64 hollow rock drill steel
Denomination | Nominal bar size mm | tolerance mm | Hole dia. incl. ovality mm | Eccentricity1) max mm | Random2) length m (±10%) | Weight kg/m |
---|---|---|---|---|---|---|
H 22 | 22.17 | +0.18/-0.17 | 6.7±0.4 | 0.6 | 7.5 - 8.5 | 3.05 |
H 25 | 25.30 | +0.30/-0.15 | 8.6±0.5 | 0.7 | 7.5 - 8.5 | 3.88 |
H 28 | 28.60 | ±0.25 | 8.8±0.5 | 0.7 | 5.5 - 6.5 | 5.05 |
H 32 | 32.05 | +0.35/-0.25 | 9.6±0.6 | 0.8 | 8 - 9 | 6.38 |
H 35 | 35.30 | ±0.30 | 9.5±0.6 | 1.0 | 9 - 10 | 7.88 |
H 38* | 38.30 | ±0.35 | 16.0±0.8 | 1.0 | 9 - 10 | 8.36 |
R 32 | 32.20 | ±0.30 | 9.2±0.5 | 0.75 | 9 - 10 | 5.87 |
R 32 | 32.20 | ±0.30 | 11.7±0.6 | 0.75 | 7.5 - 8.5 | 5.55 |
R 39 | 39.00 | ±0.30 | 10.3±0.6 | 0.8 | 6 - 7 | 8.72 |
R 39 | 39.00 | ±0.30 | 14.5±0.8 | 1.0 | 6 - 7 | 8.08 |
R 46 | 45.80 | ±0.49 | 17.0±0.9 | 1.2 | 10 - 11 | 11.15 |
R 52 | 52.05 | ±0.45 | 21.5±1.0 | 1.6 | 7 - 8 | 13.85 |
R 60 | 60.00 | ±0.70 | 22.6±2.2 | 1.75 | 7 - 8 | 19. |
1) Eccentricity = the distance between the center of the bar and the center of the hole
2) Fixed cut lengths are available on request
* Available as production order.
Denomination | Nominal bar size in. | tolerance in. | Hole dia. incl. ovality in. | Eccentricity1) max in. | Random2) length ft | Weight lb/ft |
---|---|---|---|---|---|---|
H 7/8 | 0.872 | +0.007/-0.006 | 0.263±0.015 | 0.023 | 24.6 - 27.8 | 2.05 |
H 1 | 0.996 | +0.011/-0.005 | 0.338±0.019 | 0.027 | 24.6 - 27.8 | 2.60 |
H 1 1/8 | 1.125 | ±0.009 | 0.346±0.019 | 0.027 | 18.0 - 21.3 | 3.39 |
H 1 1/4 | 1.261 | +0.012/-0.009 | 0.377±0.023 | 0.031 | 26.2 - 29.5 | 4.28 |
H 1 3/8 | 1.389 | ±0.011 | 0.374±0.023 | 0.039 | 29.5 - 32.8 | 5.29 |
H 1 1/2* | 1.507 | ±0.013 | 0.629±0.031 | 0.039 | 29.5 - 32.8 | 5.61 |
R 1 1/4 | 1.267 | ±0.011 | 0.362±0.019 | 0.029 | 29.5 - 32.8 | 3.94 |
R 1 1/4 | 1.267 | ±0.011 | 0.460±0.023 | 0.029 | 24.6 - 27.8 | 3.72 |
R 1 1/2 | 1.535 | ±0.011 | 0.405±0.023 | 0.031 | 19.6 - 22.9 | 5.85 |
R 1 1/2 | 1.535 | ±0.011 | 0.570±0.031 | 0.039 | 19.6 - 22.9 | 5.42 |
R 1 3/4 | 1.803 | ±0.015 | 0.669±0.035 | 0.047 | 32.8 - 36-0 | 7.48 |
R 2 1/32 | 2.049 | ±0.017 | 0.846±0.039 | 0.062 | 22.9 - 26.2 | 9.29 |
R 23/64 | 2.362 | ±0.027 | 0.889±0.086 | 0.068 | 22.9 - 26.2 | 12.78 |
1) Eccentricity = the distance between the center of the bar and the center of the hole
2) Fixed cut lengths are available on request
* Available as production order.