Base station PCB carrier plates in controlled expansion alloy

Need to know more?

Call us Email us

Product description

Controlled expansion alloy carrier plate expansion-matched to PCB (metal-clad laminate)

Application area

Telecom

CE alloy used

CE17 controlled expansion alloy

Material replaced

Al6061 alloy

Advantages of using CE17 controlled expansion alloy

  • Improved CTE match to PCB laminate
  • High specific stiffness