PCB guide-bars in controlled expansion alloy

Need to know more?

Call us Email us

Product description

Controlled expansion alloy guide-bars for use in robust aerospace computer systems

Application area

Computer systems

CE alloys used

CE17M controlled expansion alloy

Material replaced

W-50Cu

Advantages of using CE17M controlled expansion alloys

  • Lower price
  • 1/6 of the weight
  • 50% reduction in procurement lead-time