Resistor tubs in controlled expansion alloy

Need to know more?

Call us Email us

Product description

Lightweight resistor tub packaged in CE7 controlled expansion alloy for use in aircraft

Application area

Aerospace

CE alloy used

CE7 controlled expansion alloy

Material replaced

Plastic

Advantages of using CE7 controlled expansion alloys

Longer service life (10x) than existing plastic