Selected binary alloys incl. chemical composition (nominal), %
Alloy Fe C Cr Ni Si Mn Cu Co
Fe-Cr Bal. 0.1 1-50
-
2.0 2.0
0.5
-
Fe-Ni Bal. 0.1
-
1-50 1.0 1.0
-
-
Fe-Si Bal. 0.1
-
-
1-45 1.0
-
-
Fe-Co Bal. 0.2
-
-
1.0 1.0
-
1-50
Ni-Cr
-
0.2 1-50
Bal.
0.5 0.5
-
-
Ni-Cu
-
0.1 1-50
Bal.
0.5 0.5 1-40 3.5