Sandvik 19C27 knife steel

Excellent wear resistance
Sandvik 19C27 is Sandvik's most wear resistant knife steel grade and developed for abrasive applications. Sandvik 19C27 is the odd grade in the Sandvik knife steel portfolio because it's a coarse carbide grade, unlike the other Sandvik knife steel grades.
Buy samples of Sandvik 14C28N knife steel
Now in stock, so don't miss this opportunity!
Current availability:
- USA & Canada: Hobbyists / consumers over 18 years of age and business customers
- European Union: Hobbyists / consumers over 18 years of age and business customers
- Rest of the world: Business customers only
The coarse carbide grades excel at wear resistance but do not allow keen edge angles and have limited edge stability, due to the sacrifice of toughness related to the coarse microstructure.
Sandvik 19C27 is developed for industrial blades for cutting cardboard and tough fiber materials. The world class wear resistance is the main reason why this grade should be selected. Sandvik 19C27 is limited in corrosion resistance and we recommend surface coating on Sandvik 19C27 for knife applications to avoid corrosion issues.
With a recommended hardness range of 55-63 HRC, excellent wear resistance and a coarse carbide structure Sandvik 19C27 is suitable for industrial blades for cutting tough or/and abrasive materials.
Carbon (C) | Chromium (Cr) | Molybdenum (Mo) | Silicon (Si) | Manganese (Mn) |
---|---|---|---|---|
0.95 | 13.5 | - | 0.40 | 0.65 |