grade | Width, mm (in.) | Thickness, mm (in.) |
---|---|---|
6C27 | 5 - 380 (0.1968 - 14.96) |
0.1 - 2.5 (0.004 - 0.098) |
7C27Mo2 | 5 - 350 (0.1968 - 13.78) |
0.1 - 4.5 (0.004 - 0.177) |
12C27 | 10 - 380 (0.394 - 14.96) |
1.00 - 4.5 (0.04 - 0.177) |
12C27M | 10 - 380 (0.394 - 14.96) |
1.00 - 4.5 (0.04 - 0.177) |
13C26 | 5 - 380 (0.1968 - 14.96) |
0.1 - 3.0 (0.004 - 0.118) |
14C28N | 5 - 380 (0.1968 - 14.96) |
1.00 - 4.5 (0.04 - 0.177) |
19C27 | 5 - 340 (0.1968 - 13.38) |
0.1 - 3.0 (0.004 - 0.118) |