The table shows the size range for our knife steels. Our knife steels are delivered in coils or as straightened lengths.
Grade | Width, mm (in.) | Thickness, mm (in.) |
---|---|---|
Alleima® 6C27 | 5 - 380 (0.1968 - 14.96) |
0.1 - 2.5 (0.004 - 0.098) |
Alleima® 7C27Mo2 | 5 - 350 (0.1968 - 13.78) |
0.1 - 4.5 (0.004 - 0.177) |
Alleima®10C28Mo2 | 5-350 (0.197-13.78) |
0.074-4.5 (0.0029-0.177) |
Alleima® 12C27M | 10 - 380 (0.394 - 14.96) |
1.00 - 4.5 (0.04 - 0.177) |
Alleima® 12C27 | 10 - 380 (0.394 - 14.96) |
1.00 - 4.5 (0.04 - 0.177) |
Alleima® 13C26 | 5 - 380 (0.1968 - 14.96) |
0.1 - 3.0 (0.004 - 0.118) |
Alleima® 14C28N | 5 - 380 (0.1968 - 14.96) |
1.00 - 4.5 (0.04 - 0.177) |
Alleima® 19C27 | 5 - 340 (0.1968 - 13.38) |
0.1 - 3.0 (0.004 - 0.118) |
Alleima®10C16Mo3V1 | 15-280 (0.591-11.02) |
1.0-4.0 (0.039-0.157) |
Damax™ | 30 - 270 (1.18 - 10.63) |
2.5 - 4.0 (0.098 - 0.157) |