Shock absorber strip steel surfaces
Our strip steel for shock absorber shims is delivered bright, fine polished. The edges are slit and deburred. Shaved edges can be supplied on request.
Flatness
Maximum out-of-flatness across and along the strip is 0.30% of the nominal strip width.
Surfaces roughness
Maximum surface roughness values, cut-off 0.25 mm (0.0098 in.), are shown in the table.
Thickness
|
Ra
|
Rmax
|
|||
---|---|---|---|---|---|
mm
|
in.
|
μm
|
μin.
|
μm
|
μin.
|
≤0.508
|
≤0.020
|
0.10
|
4.0
|
1.0
|
40
|
>0.508
|
>0.020
|
0.25
|
10.0
|
2.5
|
100
|