Sandvik SAF 2507
Sandvik SAF 2507, also known as SAF 2507, is Sandvik's trademark for a super-duplex stainless steel characterized by excellent resistance to stress corrosion cracking (SCC), very high resistance to pitting and crevice corrosion, high resistance to general corrosion and very high mechanical strength.
Sandvik SAF 2507 super-duplex steel is available as tube and pipe, bar, billets and strip.
Sandvik 25.10.4.L welding wire and Sandvik 25.10.4.LR covered electrodes are specially developed welding consumables for Sandvik SAF 2507.
Material datasheets
- Sandvik SAF 2507, Seamless tube and pipe
- Sandvik SAF 2507, Bar
- Sandvik SAF 2507, Billets
- Sandvik SAF 2507, Plate and sheet
- Sandvik SAF 2507, Strip
- Sandvik SAF 2507, Wirelines