Control lines and chemical injection lines

Control lines and chemical injection lines in austenitic stainless steel and duplex stainless steel. Sandvik's range includes control lines and chemical injection lines in seamless or welded condition.
Services
Sandvik offers a quick and effective solution whether the order is for straightforward, cut to length lines or a group of lines, encapsulated, flushed and filled, supplied on customer's own reels and delivered direct to site.
Sandvik also provides coiled tubing for umbilicals.
Services
Services
Sandvik's service center in Houston (TX), US holds extensive seamless coiled tube and laser welded tube stocks for control lines and chemical injection lines to ensure just-in-time deliveries. It also operates a complete package of additional services:
- Cut to length
- Hydrotesting
- Paint striping
- Encapsulation
- Flush and fill (acc. to Nas Class 6)
- Level wound on reels
- Customer specified packaging
- Direct delivery to site
Packing standards
- Coils wound on wooden spools
- Coils wound on customer-specific metal reels
- Full package marking service, customer specific
Seamless
Seamless control lines and chemical injection lines
The tables show materials, sizes and approvals for control lines and chemical injection lines in seamless condition.
Grade | UNS | C max. | Cr | Ni | Mo | N | Others |
---|---|---|---|---|---|---|---|
TP 316L | S31600/S31603 | 0.030 | 17.5 | 13 | 2.1 | - | - |
Alloy 825 | N08825 | 0.030 | 20 | 38.5 | 2.6 | - | Cu=1.7, Ti=0.7 |
Sanicro® 28 | N08028 | 0.020 | 27 | 31 | 3.5 | - | Cu=1.0 |
Sandvik SAF 2205™ | S31803/S32205 | 0.030 | 22 | 5 | 3.2 | 0.18 | - |
Sandvik SAF 2507® | S32750 | 0.030 | 25 | 7 | 4 | 0.3 | - |
* All materials are supplied in the solution annealed condition. Other grades can be offered on request.
Grade | Yield strength, psi (MPa) |
Tensile strength, psi (MPa) |
Elongation % |
---|---|---|---|
TP 316L | 32,000 (220) | 75,000 (515) | 35 |
Alloy 825 | 35,000 (240) | 80,000 (550) | 30 |
Sanicro® 28 | 32,000 (220) | 100,000 (690) | 40 |
Sandvik SAF 2205™ | 70,000 (485) | 99,000 (680) | 25 |
Sandvik SAF 2507® | 80,000 (550) | 116,000 (800) | 25 |
1) All materials in the solution annealed condition
Grade | UNS | PRE1) | CPT2) o F (oC) |
Max. H2S3 psi | CO24) |
---|---|---|---|---|---|
TP 316L | S31600/S31603 | 24 | 95 (35) | No Limit | + |
Alloy 825 | N08825 | 29 | 140 (60) | No Limit | ++ |
Sanicro® 28 | N08028 | 39 | 150 (65) | No Limit | ++ |
Sandvik SAF 2205™ | S31803/S32205 | >35 | 150 (65) | 1.5 | + |
Sandvik SAF 2507® | S32750 | >42.5 | 195 (90) | 3 | ++ |
1) PRE = (%Cr) + 3.3 (%Mo) +16 (%N)
2) Critical Pitting Temperature in neutral solution with approximately 3% chlorides
3) Per NACE MR0175 / ISO 15156 for downhole control lines in the solution annealed condition
4) General resistance to CO2 corrosion. '++' indicates better resistance than '+'
Outside diameter | Wall thickness | Max single coil length (TP 316L) | Max single coil length (A825) |
Max LLBW1) 2) | |||
---|---|---|---|---|---|---|---|
in. | in. | m | ft | m | ft | m | ft |
1/4 | 0.035 | 252 | 827 | 640 | 2,100 | 29,000 | 95,149 |
1/4 | 0.049 | 192 | 630 | 488 | 1,601 | 22,000 | 72,182 |
1/4 | 0.065 | 158 | 518 | 401 | 1,316 | 18,000 | 59,058 |
3/8 | 0.035 | 159 | 522 | 404 | 1,326 | 18,000 | 59,058 |
3/8 | 0.049 | 118 | 387 | 300 | 984 | 14,000 | 45,934 |
3/8 | 0.065 | 94 | 308 | 239 | 784 | 11,000 | 36,091 |
3/8 | 0.083 | 78 | 256 | 199 | 653 | 9,000 | 29,529 |
1/2 | 0.035 | 116 | 381 | 296 | 971 | 13,000 | 24,653 |
1/2 | 0.049 | 85 | 279 | 217 | 712 | 10,000 | 32,810 |
1/2 | 0.065 | 67 | 220 | 171 | 561 | 7,500 | 24,608 |
1/2 | 0.083 | 55 | 180 | 139 | 456 | 6,000 | 19,686 |
5/8 | 0.035 | 92 | 302 | 234 | 767 | 10,750 | 35,271 |
5/8 | 0.049 | 67 | 220 | 171 | 561 | 7,500 | 24,608 |
5/8 | 0.065 | 52 | 171 | 131 | 430 | 6,100 | 20,014 |
5/8 | 0.083 | 25 | 82 | 25 | 82 | 5,000 | 16,405 |
3/4 | 0.035 | 25 | 82 | 25 | 82 | - | - |
3/4 | 0.049 | 25 | 82 | 25 | 82 | - | - |
3/4 | 0.065 | 25 | 82 | 25 | 82 | - | - |
3/4 | 0.083 | 25 | 82 | 25 | 82 | - | - |
1) Long length butt welded
2) For 3/4 in. OD single coils can be made. Contact us for complete details.
Approvals
- ISO 9001:2000
- ISO 14001:2004
- OHSAS 18001
- PED 97/23/EC
- ANSI NACE MR 0175 / ISO 15156
Welded
Welded control lines and chemical injection lines
The tables show materials, sizes and approvals for control lines and chemical injection lines in welded condition.
Grade | UNS | C max. |
Cr | Ni | Mo | Others |
---|---|---|---|---|---|---|
TP 316L | S31600/S31603 | 0.030 | 17.5 | 13 | 2.1 | 0.1 |
Alloy 825 | N08825 | 0.030 | 20 | 38.5 | 2.6 | Cu=1.7, Ti=0.7 |
Alloy 625 | N6625 | 0.10 | 21.5 | >=58 | 9 | Nb=3.5 |
*All materials are supplied in the solution annealed condition. Other grades can be offered on request.
Grade | Yield strength, psi (MPa) |
Tensile strength, psi (MPa) |
Elongation % |
---|---|---|---|
TP 316L | 32,000 (220) | 75,000 (515) | 35 |
Alloy 825 | 35,000 (240) | 80,000 (550) | 30 |
Alloy 625 | 60,000 (415) | 110,000 (760) | 30 |
1) All materials in the solution annealed condition
Grade | UNS | PRE1) | CPT2) F (oC) | Max H2S3) psi | CO24) |
---|---|---|---|---|---|
TP 316L | S31600/S31603 | 24 | 95 (35) | No limit | + |
Alloy 825 | N08825 | 29 | 140 (60) | No limit | ++ |
Alloy 625 | N06625 | 52 | 195 (90) | No limit | ++ |
1) PRE = (%Cr) + 3.3 (%Mo) +16 (%N)
2) Critical Pitting Temperature in neutral solution with approximately 3% chlorides
3) Per NACE MR0175 / ISO 15156 for downhole control lines in the solution annealed condition
4) General resistance to CO2 corrosion. '++' indicates better resistance than '+'
Size range (in.)
The table shows stock standard sizes. Other sizes can be offered on request.
OD | WT | OD | WT | OD | WT | OD | WT | OD | WT |
---|---|---|---|---|---|---|---|---|---|
1/4 | 0.035 | 3/8 | 0.035 | 1/2 | 0.035 | 5/8 | 0.035 | 3/4 | 0.035 |
1/4 | 0.049 | 3/8 | 0.049 | 1/2 | 0.049 | 5/8 | 0.049 | 3/4 | 0.049 |
1/4 | 0.065 | 3/8 | 0.065 | 1/2 | 0.065 | 5/8 | 0.065 | 3/4 | 0.065 |
- | - | 3/8 | 0.083 | 1/2 | 0.083 | 5/8 | 0.083 | 3/4 | 0.083 |
OD = Outside diameter, WT = Wall thickness
Approvals
- ISO 9001:2000
- Intertek
- MGMT. SYS. RvA 050
- ANAB
Encapsulation
Encapsulation materials
Sandvik offers a wide range of encapsulation materials. The most frequent ones can be found in the table below. Other encapsulation materials can be offered upon request.
Material rating on a scale of 1 to 5 (1=not good, 5=excellent)
Materials | Max temp. oF (Co) |
Abrasion resistance | Resistance to inhibited brine well fluids | Resistance to oil/diesel well fluids |
---|---|---|---|---|
Polypropylene | 150 (65) | 2 | 5 | 3 |
Nylon 11 | 200 (93) | 4 | 3 | 3 |
PVC | 174 (79) | 3 | 2 | 3 |
TPV | 275 (135) | 3 | 5 | 3 |
Halar | 300 (149) | 4 | 4 | 5 |
PVDF | 310 (154) | 4 | 3 | 5 |
MPH340G | 340 /171) | 4 | 4 | 5 |
Pressure tables
Pressure tables
Selection of the appropriate material for any given control or chemical injection line is subject to the prevailing operational and site conditions. In order to assist in the selection, the following tables provide internal pressure ratings and the adjustments factors for a range of common grades and sizes of seamless and laser welded stainless tubing.
Maximum pressure (P) for TP 316L at 100°F (38°C)1)
Please refer to grade and product form adjustment factors below.
Outside diameter, in. | Wall thickness, in. | Working pressure2) psi (MPa) |
Burst pressure2) psi (MPa) |
Collapse pressure4) psi (MPa) |
---|---|---|---|---|
1/4 | 0.035 | 6,600 (46) | 22,470 (155) | 6,600 (46) |
1/4 | 0.049 | 9,260 (64) | 27,400 (189) | 8,710 (60) |
1/4 | 0.065 | 12,280 (85) | 34,640 (239) | 10,750 (74) |
3/8 | 0.035 | 4,410 (30) | 19,160 (132) | 4,610 (32) |
3/8 | 0.049 | 6,170 (43) | 21,750 (150) | 6,220 (43) |
3/8 | 0.065 | 8,190 (56) | 25,260 (174) | 7,900 (54) |
3/8 | 0.083 | 10,450 (72) | 30,050 (207) | 9,570 (66) |
1/2 | 0.049 | 4,630 (32) | 19,460 (134) | 4,820 (33) |
1/2 | 0.065 | 6,140 (42) | 21,700 (150) | 6,200 (43) |
1/2 | 0.083 | 7,840 (54) | 24,600 (170) | 7,620 (53) |
5/8 | 0.049 | 3,700 (26) | 18,230 (126) | 3,930 (27) |
5/8 | 0.065 | 4,900 (34) | 19,860 (137) | 5,090 (35) |
5/8 | 0.083 | 6,270 (43) | 26,910 (151) | 6,310 (44) |
3/4 | 0.049 | 3,080 (21) | 17,470 (120) | 3,320 (23) |
3/4 | 0.065 | 4,090 (28) | 18,740 (129) | 4,310 (30) |
3/4 | 0.083 | 5,220 (36) | 20,310 (140) | 5,380 (37) |
1) Estimates only. Actual pressures should be calculated considering all stress factors in the system.
2) Based on calculations from API 5C3, using a wall tolerance of +/-10%
3) Based on ultimate strength burst calculations from API 5C3
4) Based on yield strength collapse calculations from API 5C3
Adjustment factors for working pressure limits1)
Pw = reference working pressure rating for TP 316L at 100°F (38°C). To determine working pressure for grade/temperature combination, multiply Pw by adjustment factor.
Grade | 100°F (38°C) |
200°F (93°C) |
300°F (149°C) |
400°F (204°C) |
---|---|---|---|---|
TP 316L, seamless | 1.00 | 0.87 | 0.70 | 0.63 |
TP 316L, welded | 0.85 | 0.74 | 0.60 | 0.54 |
Sandvik SAF 2205™, seamless | 2.17 | 2.00 | 1.77 | 1.60 |
Sandvik SAF 2205™, welded | 1.84 | 1.70 | 1.50 | 1.36 |
Alloy 825, seamless | 1.33 | 1.17 | 1.10 | 1.03 |
Alloy 825, welded | 1.13 | 0.99 | 0.94 | 0.88 |
Sandvik SAF 2507® , seamless | 2.67 | 2.33 | 2.17 | 1.70 |
Sandvik SAF 2507® , welded | 2.27 | 1.98 | 1.84 | 1.45 |
1) Adjustment factors based on allowable stress in ASME.
Example: The maximum factors allowable working pressure for seamless 1/2 x 0.049 in. Sandvik SAF 2507® tubing at 100°F (38°C) can be calculated as:
4,630 psi – Pressure rating for TP 316L at 100°F (38°C)
x 2.67 – Adjustment factor for Sandvik SAF 2507, seamless at 100°F (38°C)
12,362 psi – Working pressure rating for Sandvik SAF 2507® tubing
Adjustment factors for burst pressure limits1)
Pb = reference burst pressure for TP 316L at 100°F. To determine burst pressure for grade/temperature combination, multiply Pb by adjustment factor.
Grade | 100°F (38°C) |
200°F (93°C) |
300°F (149°C) |
400°F (204°C) |
---|---|---|---|---|
TP 316L, seamless | 1.00 | 0.93 | 0.87 | 0.80 |
TP 316L, welded | 0.85 | 0.79 | 0.74 | 0.68 |
Sandvik SAF 2205™, seamless | 1.71 | 1.33 | 1.20 | 1.07 |
Sandvik SAF 2205™, welded | 1.45 | 1.13 | 1.02 | 0.91 |
Alloy 825, seamless | 1.13 | 1.07 | 1.00 | 0.87 |
Alloy 825, welded | 0.96 | 0.91 | 0.85 | 0.74 |
Sandvik SAF 2507® , seamless | 1.97 | 1.75 | 1.57 | 1.35 |
Sandvik SAF 2507® , welded | 1.64 | 1.47 | 1.31 | 1.13 |
1) Adjustment factors based on ultimate strength in ASME.
Example: The maximum factors burst pressure for seamless 3/8 x 0.049 in. Sandvik SAF 2507® tubing at 200°F (93°C) can be calculated as:
21,750 psi – burst pressure rating for TP 316L at 100°F (38°C)
x 1.73 – Adjustment factor for Sandvik SAF 2507, seamless at 200°F (93°C)
37,627 psi – burst pressure rating for Sandvik SAF 2507® tubing
Adjustment factors for collapse pressure limits1)
Pc = reference collapse pressure rating for TP 316L at 100°F (38°C). To determine collapse pressure for grade/temperature combination, multiply Pc by adjustment factor.
Grade | 100°F (38°C) |
200°F (93°C) |
300°F (149°C) |
400°F (204°C) |
---|---|---|---|---|
TP 316L, seamless | 1.00 | 0.87 | 0.70 | 0.63 |
TP 316L, welded | 0.85 | 0.74 | 0.60 | 0.54 |
Sandvik SAF 2205™, seamless | 2.17 | 2.00 | 1.77 | 1.60 |
Sandvik SAF 2205™, welded | 1.84 | 1.70 | 1.50 | 1.36 |
Alloy 825, seamless | 1.33 | 1.17 | 1.10 | 1.03 |
Alloy 825, welded | 1.13 | 0.99 | 0.94 | 0.88 |
Sandvik SAF 2507® , seamless | 2.67 | 2.33 | 2.17 | 1.70 |
Sandvik SAF 2507® , welded | 2.27 | 1.98 | 1.84 | 1.45 |
1) Adjustment factors based on yield strength in ASME.
Example: The maximum factors collapse pressure for seamless 1/4 x 0.035 in. Alloy 825 tubing at 200°F (93°C) can be calculated as:
6,600 psi – Collapse pressure rating for ASTM 316L at 100°F (38°C)
x 1.17 – Adjustment factor for Alloy 825 seamless at 200°F (93°C)
7,722 psi – Collapse pressure rating for Alloy 825 tubing