Tube, pipe, fittings and flanges
Heat exchanger tube in an extensive range of austenitic stainless steels, duplex stainless steels, nickel alloys, titanium and zirconium, suitable for all types of heat exchangers, such as seawater coolers, condensers, evaporators, heaters and reheaters.
Our heat exchanger tube portfolio includes imperial and metric sizes, from outside diameter 12 mm up to 40 mm (0.472 to 1.575 in.). Special sizes can be made to order. Alleima heat exchanger tubes are supplied in straight lengths up to 30 meters, or as U-bent tubes.
Our portfolio of duplex stainless steels is the widest on the market. Duplex stainless steel heat exchanger tubes perform exceptionally well in a variety of environments and media common in process industries, resulting in lower life-cycle costs.
One of the latest developments in the Alleima duplex family, SAF™ 2707 HD™ hyper-duplex stainless steel, can serve as a very competitive alternative to expensive nickel alloys and high-alloy austenitic stainless steels in the most demanding applications.
The tables show our standard materials for heat exchanger tube. Other grades can be offered on request.
Alleima grade | UNS | ASTM | EN no. | W.-nr | AFNOR |
---|---|---|---|---|---|
Alleima® 3RE60 | S31500 | - | 1.4424 | 1.4417 | Z2CND18-05-03 |
SAF™ 2205 | S31803/S32205 | - | 1.4462 | - | Z2CND22-05-03 |
SAF™ 2304 | S32304 | - | 1.4362 | 1.4362 | Z2NC23-04AZ |
SAF™ 2707 HD | S32707 | - | - | - | - |
SAF™ 2507 | S32750 | - | 1.4410 | - | - |
Alleima grade | UNS | ASTM | EN steel no. | W.-nr | AFNOR |
---|---|---|---|---|---|
Sanicro® 70 | N06600 | Alloy 600 | - | 2.4816 | - |
Sanicro® 69 | N06690 | Alloy 690 | 2.4642*** | 2.4642 | NC30FE(RCCM) |
Sanicro® 625 | N06625 | Alloy 625 | - | - | - |
Sanicro® 41 | N08825 | Alloy 825 | - | 2.4858 | - |
Sanicro® 35 | N08935 | - | - | - | - |
Sanicro® 30 | N08800 | - | 1.4558 | 1.4558 | - |
Sanicro® 28 | N08028 | - | 1.4563 | 1.4563 | - |
Alleima® 2RK65 | N08904 | - | 1.4539 | 1.4539 | Z1NCDU25-20-4 |
254 SMO* | S31254 | - | 1.4547 | (1.4529)** | - |
* 254 SMO is a trademark of Outokumpu OY.
** In brackets, nearest equivalent steel grade
*** Not applicable for tube and pipe. Only for information.
Alleima grade | UNS | ASTM | EN steel no. | W.-nr | AFNOR |
---|---|---|---|---|---|
Alleima® 3R12 | S30403/S30400 | 304L/304 | 1.4306/1.4301 | 1.4306/1.4301 | Z2CN18-10 |
Alleima® 3R60 | S31603/S31600 | 316L/316 | 1.4435/1.4436 | 1.4435/1.4436 | Z2CND17-13 |
Alleima® 5R75 | S31635 | 316Ti | 1.4571 | 1.4571 | (Z6CNDT17-12)** |
Alleima® 6R35 | S32100/S32109 | 321/321H | 1.4541/1.4940 | 1.4541/1.4878 | (Z6CNT18-10)** |
Type of material | Grade(s) |
---|---|
Titanium | Pure titanium and titanium grades: 1, 2, 3, 4, 7, 9, 11, 12, 16, 17, 26 and 28 |
Zirconium | Zirconium 702 (ZR-702) |
American standards | European standards | |||
---|---|---|---|---|
Alleima grade | ASTM | ASME | EN | VD TÜV |
Duplex | ||||
SAF™ 2707 HD | A-789 | SA-789 | - | - |
SAF™ 2507 | A-789 | SA-789 | 10216-5 | VD TÜV Blatt 508 |
SAF™ 2205 | A-789 | SA-789 | 10216-5 | VD TÜV Blatt 418 |
SAF™ 2304 | A-789 | SA-789 | 10216-5 | - |
Alleima® 3RE60 | A-789 | SA-789 | - | - |
Ni-Alloy | ||||
Sanicro® 70 | B-163 B-167 | SB-163 SB-167 | - | VD TÜV Blatt 305 |
Sanicro® 69 | B-163 B-167 | SB-163 SB-167 | - | - |
Sanicro® 41 | B-163 B-423 | SB-163 SB-423 | - | - |
Sanicro® 35 | B-163 | SB-163 | - |
TUV 1326W043219 |
Sanicro® 30 | B-163 B-407 | SB-163 SB-407 | 10216-5 | - |
Sanicro® 28 | B-668 | SB-668 | 10216-5 | VD TÜV Blatt 483 |
Alleima® 2RK65 | A-269 | SB-677 | 10216-5 | VD TÜV Blatt 421 |
254 SMO* | A-213 A-269 | SA-213 SA-269 | 10216-5 | - |
Austenitic | ||||
Alleima® 5R75 | A-213 | SA-213 | 10216-5 | - |
Alleima® 3R60 | A-213 A-269 | SA-213 | 10216-5 | - |
Alleima® 3R65 | A-213 A-269 | SA-213 | 10216-5 | - |
Alleima® 6R35 | A-213 A-269 | SA-213 | 10216-5 | - |
Alleima® 3R12 | A-213 A-269 | SA-213 | 10216-5 | - |
Alleima grade | UNS |
Proof strength
|
Tensile strength
|
Elongation
|
---|---|---|---|---|
Rp0.2 | Rm | A | ||
MPa/ksi | MPa/ksi | % | ||
min. | min. | |||
Duplex stainless steels | ||||
SAF™ 2707 HD | UNS S32707 |
700*/116*
|
920-1,000/133-160*
|
25
|
SAF™ 2507 | UNS S32750 |
550/93
|
800-1,000/116-145
|
25
|
SAF™ 2205 | UNS S31803/S32205 |
485/73
|
680-880/99-128
|
25
|
SAF™ 2304 | UNS S32304 |
400/65
|
600-820/87-119
|
25
|
Alleima® 3RE60 | UNS S31500 |
450
|
700-800/
|
- |
Nickel alloys and high-alloy austenitic stainless steels | ||||
Sanicro® 70 | UNS N06600 |
245
|
>560
|
35
|
Sanicro® 69 | UNS N06690 |
240
|
585
|
30
|
Sanicro® 41 | UNS N08825 |
240
|
590-750
|
30
|
Sanicro® 30 | UNS N08800 | 205 | 520-690 | 30 |
Sanicro® 28 | UNS N08028 |
220
|
550-750
|
40
|
Alleima® 2RK65 | UNS N08904 |
230
|
520-720
|
35
|
254 SMO* | UNS S31254 |
310
|
655-850
|
35
|
Austenitic stainless steels | ||||
Alleima® 5R75 | UNS S31635 |
220
|
510-710
|
35
|
Alleima® 3R60 | UNS S31603/S31600 |
220
|
515-690
|
45
|
Alleima® 6R35 | UNS S32100/S32109 |
210
|
515-690
|
35
|
Alleima® 3R12 | UNS S30403/S30400 |
210
|
515-680
|
45
|
Alleima stainless heat exchanger tubes can also be delivered as U-bent tubes*, manufactured according to the common heat exchanger standards. Our basic specification is Alleima spec. 7-2-1179, but we can also use DIN 28179, TEMA RCB 2.31 or various customer specifications. Copies of all specifications are available on request.
If specified, we are equipped to carry out heat treatment of bends plus minimum 150 mm of leg.
* Valid for wall thickness less than or equal to 4 mm/0.157 in.