End caps, butt weld fittings

Need to know more?

Call us Email us

ASTM A403 / A815 ASME B16.9

Product code example:

●: FBEC-316L-1-10S
●: FBEC-W31803-3-10S

● = stock standard, made from plate

Nominal pipe sizeSch.*Dimensions in mm WeightASTMASTMUNS
in. DtEkg/pce304/304L316/316LS31803
1/2 10s
40s
80s
21.3
21.3
21.3
2.11
2.77
3.73
25.4
25.4
25.4
0.040
0.050
0.050


-



-
-
3/4 10s
40s
80s
26.7
26.7
26.7
2.11
2.87
3.91
25.4
25.4
25.4
0.050
0.060
0.060


-




-
1 10s
40s
80s
33.4
33.4
33.4
2.77
3.38
4.55
38.1
38.1
38.1
0.090
0.130
0.130


-




-
10s
40s
80s
42.2
42.2
42.2
2.77
3.56
4.85
38.1
38.1
38.1
0.130
0.170
0.180


-


-
-
-
10s
40s
80s
48.3
48.3
48.3
2.77
3.68
5.08
38.1
38.1
38.1
0.140
0.230
0.240


-




-
2 10s
40s
80s
60.3
60.3
60.3
2.77
3.91
5.54
38.1
38.1
38.1
0.170
0.270
0.340


-




-
10s
40s
80s
73.0
73.0
73.0
3.05
5.16
7.01
38.1
38.1
38.1
0.250
0.450
0.510


-




-
3 10s
40s
80s
88.9
88.9
88.9
3.05
5.49
7.62
50.8
50.8
50.8
0.400
0.710
0.850






4 10s
40s
80s
114.3
114.3
114.3
3.05
6.02
8.56
63.5
63.5
63.5
0.650
1.220
1.610






-
5 10s
40s
80s
141.3
141.3
141.3
3.40
6.55
9.53
76.2
76.2
76.2
1.020
1.910
2.550


-



-
-
6 10s
40s
80s
168.3
168.3
168.3
3.40
7.11
10.97
88.9
88.9
88.9
1.360
3.230
4.540


-




-
8 10s
40s
219.1
219.1
3.76
8.18
101.6
101.6
2.490
5.670



10 10s
40s
273.1
273.1
4.19
9.27
127.0
127.0
4.900
9.210



-
12 10s
40s
323.9
323.9
4.57
9.53
152.4
152.4
6.530
13.060



-
14 10s
STD
355.6
355.6
4.78
9.53
165.1
165.1
8.160
15.900

-

-
-
16 10s
STD
406.4
406.4
4.78
9.53
177.8
177.8
14.510
20.000

-

-
-
18 10s 457.2 4.78 203.2 17.960 -
20 10s 508.0 5.54 228.6 27.220 -
24 10s 609.6 6.35 266.7 34.470 -