Eccentric reducers, butt weld fittings

Need to know more?

Call us Email us

ASTM A403 / ASME B16.9

Product code example:

●: FBRE-304L-2-1-10S
▲: FBRE-W316L-8-4-10S

● = stock standard, made from seamless pipe
▲ = stock standard, made from welded pipe or plate

Nominal pipe sizeSch.*Dimensions in mmWeightASTMASTM
in. DD1tt1Hkg/pce304/304L316/316L
3/4  x 1/2 10s
40s
80s
26.7
26.7
26.7
21.3
21.3
21.3
2.11
2.87
3.91
2.11
2.77
3.73
39.3
39.3
39.3
0.100
0.140
0.075
●/▲

-
●/▲

1  x 1/2 10s
40s
80s
33.4
33.4
33.4
21.3
21.3
21.3
2.77
3.38
4.55
2.11
2.77
3.73
50.8
50.8
50.8
0.120
0.150
0.133
●/▲
●/▲
-
●/▲
●/▲
1  x 3/4 10s
40s
80s
33.4
33.4
33.4
26.7
26.7
26.7
2.77
3.38
4.55
2.11
2.87
3.91
50.8
50.8
50.8
0.130
0.160
0.147
●/▲
●/▲´
-
●/▲
●/▲
1/4  x 3/4 10s 42.2 26.7 2.77 2.11 50.8 0.180 -
1¼ x 1 10s
40s
80s
42.2
42.2
42.2
33.4
33.4
33.4
2.77
3.56
4.85
2.77
3.38
4.55
50.8
50.8
50.8
0.180
0.220
0.206


-


1½ x 1/2 40s 48.3 21.3 3.68 2.77 63.5 0.183 -
1½ x 3/4 10s
40s
80s
48.3
48.3
48.3
26.7
26.7
26.7
2.77
3.68
5.08
2.11
2.87
3.91
63.5
63.5
63.5
0.200
0.260
0.180


-
●/▲

1½ x 1 10s
40s
80s
48.3
48.3
48.3
33.4
33.4
33.4
2.77
3.68
5.08
2.77
3.68
4.55
63.5
63.5
63.5
0.200
0.260
0.291
●/▲
●/▲
-
●/▲
●/▲
1½ x 1¼ 10s
40s
80s
48.3
48.3
48.3
42.2
42.2
42.2
2.77
3.68
5.08
2.77
3.56
4.85
63.5
63.5
63.5
0.210
0.280
0.324
-
-
-


2  x 3/4 80s 60.3 26.7 5.54 3.91 76.2 0.406 -
2  x 1 10s
40s
80s
60.3
60.3
60.3
33.4
33.4
33.4
2.77
3.91
5.54
2.77
3.38
4.55
76.2
76.2
76.2
0.280
0.400
0.438
●/▲
●/▲
-
●/▲
●/▲
2  x 1¼ 10s
80s
60.3
60.3
42.2
42.2
2.77
5.54
2.77
4.85
76.2
76.2
0.300
0.478

-

2  x 1½ 10s
40s
80s
60.3
60.3
60.3
48.3
48.3
48.3
2.77
3.91
5.54
2.77
3.68
5.08
76.2
76.2
76.2
0.310
0.450
0.508
●/▲
●/▲
●/▲
●/▲
3  x 1 40s 88.9 33.4 5.49 3.38 88.9 0.850 -
3  x 1½ 10s
40s
88.9
88.9
48.3
48.3
3.05
5.49
2.77
3.68
88.9
88.9
0.510
0.940
●/▲
●/▲
●/▲
●/▲
3  x 2 10s
40s
88.9
88.9
60.3
60.3
3.05
5.49
2.77
3.91
88.9
88.9
0.550
1.000
●/▲
●/▲
●/▲
●/▲
3  x 2½ 10s
40s
88.9
88.9
73.0
73.0
3.05
5.49
2.77
5.16
88.9
88.9
0.590
1.080
●/▲
●/▲
4  x 1½ 10s 114.3 48.3 3.05 2.77 101.6 0.629 -
4  x 2 10s
40s
114.3
114.3
60.3
60.3
3.05
6.02
2.77
3.91
101.6
101.6
0.780
1.570
●/▲
●/▲
●/▲
●/▲
4  x 2½ 10s
40s
114.3
114.3
73.0
73.0
3.05
6.02
3.05
5.16
101.6
101.6
0.830
1.660
●/▲
●/▲
4  x 3 10s
40s
114.3
114.3
88.9
88.9
3.05
6.02
3.05
5.49
101.6
101.6
0.870
1.740
●/▲
●/▲
●/▲
●/▲
5  x 3 10s
40s
141.3
141.3
88.9
88.9
3.40
6.55
3.05
5.49
127.0
127.0
1.450
2.850

-

5  x 4 10s
40s
141.3
141.3
114.3
114.3
3.40
6.55
3.05
6.02
127.0
127.0
1.490
2.980
-
-

6  x 3 10s
40s
168.3
168.3
88.9
88.9
3.40
7.11
3.05
5.49
139.7
139.7
1.820
3.980
●/▲
●/▲
6  x 4 10s
40s
168.3
168.3
114.3
114.3
3.40
7.11
3.05
6.02
139.7
139.7
1.950
4.080
●/▲
●/▲
●/▲
6  x 5 10s
40s
168.3
168.3
141.3
141.3
3.40
7.11
3.40
6.55
139.7
139.7
2.000
4.150
-
-

8  x 4 10s
40s
219.1
219.1
114.4
114.4
3.76
8.18
3.05
6.02
152.4
152.4
3.020
6.550
●/▲
●/▲
●/▲
●/▲
8  x 5 10s
40s
219.1
219.1
141.3
141.3
3.76
8.18
3.05
6.02
152.4
152.4
3.080
6.700


8  x 6 10s
40s
219.1
219.1
168.3
168.3
3.76
8.18
3.40
7.11
152.4
152.4
3.190
6.940
●/▲
●/▲
●/▲
●/▲
10  x 6 10s
40s
273.1
273.1
168.3
168.3
4.19
9.27
3.40
7.11
177.8
177.8
5.000
11.120


10  x 8 10s
40s
273.1
273.1
219.1
219.1
4.19
9.27
3.76
8.18
177.8
177.8
5.250
11.560


12  x 6 10s
40s
323.9
323.9
168.3
168.3
4.57
9.53
3.40
7.11
203.2
203.2
7.450
11.120


12  x 8 10s
40s
323.9
323.9
219.1
219.1
4.57
9.53
3.76
8.18
203.2
203.2
7.670
15.980


12  x 10 10s
40s
323.9
323.9
273.1
273.1
4.57
9.53
4.19
9.27
203.2
203.2
7.980
16.630


14  x 8 10s 355.6 219.1 4.78 3.76 330.2 13.880 -
14  x 10 10s 355.6 273.1 4.78 4.19 330.2 14.410
14  x 12 10s 355.6 323.9 4.78 4.57 330.2 15.290
16  x 10 10s 406.4 273.1 4.78 4.19 355.6 17.720
16  x 12 10s 406.4 323.9 4.78 4.57 355.6 18.350

* Schedule