Reducing tees, butt weld fittings

Need to know more?

Call us Email us

ASTM A403 / A815 ASME B16.9

Product code example:

●: FBRT-304L-4-2-10S
▲: FBRT-W316L-10-6-10S

● = stock standard, made from seamless pipe
▲ = stock standard, made from welded pipe or plate

Nom pipe size, in.Sch*Dimensions in mmWeightASTMASTM
RunOutlet DD1tt1CMkg/pce304L316L
3/4
1/2
10s
40s
80s
26.7
26.7
26.7
21.3
21.3
21.3
2.11
2.87
3.91
2.11
2.77
3.73
29
29
29
29
29
29
0.110
0.150
0.190

-
●/▲

1
1/2
10s
40s
80s
33.4
33.4
33.4
21.3
21.3
21.3
2.77
3.38
4.55
2.11
2.77
3.73
38
38
38
38
38
38
0.190
0.220
0.281
●/▲

●/▲

1
3/4
10s
40s
80s
33.4
33.4
33.4
26.7
26.7
26.7
2.77
3.38
4.55
2.11
2.87
3.91
38
38
38
38
38
38
0.190
0.230
0.270
●/▲
-
●/▲

1/2
40s 42.2 21.3 3.56 2.77 47.6 47.6 0.367
3/4
10s
40s
42.2
42.2
26.7
26.7
2.77
3.56
2.11
2.87
47.6
47.6
47.6
47.6
0.440
0.530
-

1
10s
40s
80s
42.2
42.2
42.2
33.4
33.4
33.4
2.77
3.56
4.85
2.77
3.38
4.55
47.6
47.6
47.6
47.6
47.6
47.6
0.450
0.530
0.600

-
●/▲

1/2
10s
40s
48.3
48.3
21.3
21.3
2.77
3.68
2.11
2.77
57
57
57
57
0.390
0.520

●/▲
3/4
10s
40s
80s
48.3
48.3
48.3
26.7
26.7
26.7
2.77
3.68
5.08
2.11
2.87
3.91
57
57
57
57
57
57
0.390
0.520
0.690
-
-


1
10s
40s
80s
48.3
48.3
48.3
33.4
33.4
33.4
2.77
3.68
5.08
2.77
3.38
4.55
57
57
57
57
57
57
0.420
0.550
0.724
●/▲

●/▲

2
3/4
10s
40s
80s
60.3
60.3
60.3
26.7
26.7
26.7
2.77
3.91
5.54
2.11
2.87
3.91
64
64
64
44
44
44
0.510
0.710
0.990

-


2
1
10s
40s
80s
60.3
60.3
60.3
33.4
33.4
33.4
2.77
3.91
5.54
2.77
3.38
4.55
64
64
64
51
51
51
0.540
0.740
1.020
●/▲



2
10s
40s
80s
60.3
60.3
60.3
42.2
42.2
42.2
2.77
3.91
5.54
2.77
3.56
4.85
64
64
64
57
57
57
0.571
0.804
1.07

-
-
-
2
10s
40s
60.3
60.3
48.3
48.3
2.77
3.91
2.77
3.68
64
64
60
60
0.590
0.830
●/▲
●/▲
10s 73.0 42.2 3.05 2.77 76 67 0.874
-
10s
40s
73.0
73.0
48.3
48.3
3.05
5.16
2.77
3.68
76
76
67
67
0.900
1.490
●/▲

●/▲
2 10s
40s
73.0
73.0
60.3
60.3
3.05
5.16
2.77
3.91
76
76
70
70
0.940
1.530
●/▲
-
●/▲
3 1 10s
40s
88.9
88.9
33.4
33.4
3.05
5.49
2.77
3.38
86
86
73
73
1.150
2.050


3 10s
40s
88.9
88.9
48.3
48.3
3.05
5.49
2.77
3.68
86
86
73
73
1.190
2.050
●/▲
●/▲
3 2 10s
40s
88.9
88.9
60.3
60.3
3.05
5.49
2.77
3.91
86
86
76
76
1.230
2.160
●/▲
●/▲
3 10s
40s
88.9
88.9
73.0
73.0
3.05
5.49
3.05
5.16
86
86
83
83
1.310
2.290
●/▲
-
●/▲
4 10s
40s
114.3
114.3
48.3
48.3
3.05
6.02
2.77
3.68
105
105
86
86
1.750
4.000
-
-


4 2 10s
40s
114.3
114.3
60.3
60.3
3.05
6.02
2.77
3.91
105
105
89
89
2.000
4.500
●/▲
●/▲
4 10s
40s
114.3
114.3
73.0
73.0
3.05
6.02
3.05
5.16
105
105
95
95
2.100
4.700

-
●/▲
4 3 10s
40s
114.3
114.3
88.9
88.9
3.05
6.02
3.05
5.49
105
105
98
98
2.150
5.000
●/▲
●/▲
5 3 10s
40s
141.3
141.3
88.9
88.9
3.40
6.55
3.05
5.49
124
124
111
111
3.130
7.500
-
-

5 4 10s
40s
141.3
141.3
114.3
114.3
3.40
6.55
3.05
6.02
124
124
117
117
3.260
8.000
-
-
●/▲
6 10s 168.3 73.0 3.40 3.05 143 124 5.000 -
6 3 10s
40s
168.3
168.3
88.9
88.9
3.40
7.11
3.05
5.49
143
143
124
124
4.900
11.000
●/▲
●/▲
6 4 10s
40s
168.3
168.3
114.3
114.3
3.40
7.11
3.05
6.02
143
143
130
130
5.100
11.500
●/▲
●/▲
6 5 10s
40s
168.3
168.3
141.3
141.3
3.40
7.11
3.40
6.55
143
143
137
137
5.300
12.000

-

8 4 10s
40s
219.1
219.1
114.3
114.3
3.76
8.18
3.05
6.02
178
178
156
156
7.700
20.500
●/▲
●/▲
●/▲
●/▲
8 5 10s
40s
219.1
219.1
141.3
141.3
3.76
8.18
3.40
6.55
178
178
162
162
8.150
20.700
-

8 6 10s
40s
219.1
219.1
168.3
168.3
3.76
8.18
3.40
7.11
178
178
168
168
8.300
21.000
●/▲
●/▲
●/▲
●/▲
10 4 10s
40s
273.1 
273.1
114.3
114.3
4.19
9.27 
3.05
6.02
216
216 
184
184
13.000
35.000 

-

10  10s
40s
273.1 
273.1
168.3
168.3
4.19
9.27
3.40
7.11
216
216
194
194 
16.500
36.000 

●/▲
●/▲
10  10s
40s
273.1 
273.1
219.1
219.1
4.19
9.27 
3.76
8.18
216
216
203
203 
16.700
36.300 
●/▲
●/▲
●/▲
●/▲
12 6 10s
40s
323.9
323.9
168.5
168.5
4.57
9.53
3.40
7.11
254
254 
219
219 
23.000
52.000 

●/▲

12 8 10s
40s
323.9
323.9
219.1
219.1 
4.57
9.53
3.76
8.18
254
254
229
229 
24.000
53.000 
●/▲

12 10 10s
40s
323.9
323.9
273.1
273.1 
4.57
9.53
3.76
9.27 
254
254
241
241 
25.000
54.000 
●/▲

* Schedule