Couplings, socket weld

Need to know more?

Call us Email us

ASTM A182 3000 lbs ASME B16.11 / BS 3799

Product code example:

FSCO-316L-1/4-3000

● = stock standard

Nominal pipe size B L1 C D E
Weight
ASTM
ASTM
in. mm socket mm mm mm ~kg/pce 304/304L 316/316L
1/4
3/8
1/2
3/4
14.20
17.60
21.80
27.20
9.53
9.53
9.53
12.50
3.30
3.51
4.09
4.27
8.86
12.14
15.42
20.55
6.35
6.35
9.53
9.53
0.05
0.10
0.14
0.20






1


2
33.90
42.70
48.80
61.20
12.50
12.50
12.50
16.00
4.98
5.28
5.54
6.05
26.26
34.67
40.51
52.12
12.70
12.70
12.70
19.05
0.30
0.45
0.60
0.95