Couplings, NPT-threaded
ASTM A182 3000 lbs, ASME B16.11 / BS 3799
Full couplings
Product code example:
FTCO-316L-1/4-3000
● = stock standard
Nominal pipe size | L | D | B |
Weight
|
ASTM
|
ASTM
|
---|---|---|---|---|---|---|
in. | mm | mm | mm | ~kg/pce | 304/304L | 316/316L |
1/4 3/8 1/2 3/4 |
34.9
38.1 47.6 50.8 |
19.1
22.2 28.6 34.9 |
8.13
9.14 10.92 12.70 |
0.05
0.06 0.14 0.20 |
●
● ● ● |
●
● ● ● |
1 1 ¼ 1 ½ 2 |
60.3
66.7 79.4 85.7 |
44.5
57.6 63.5 76.2 |
14.73
17.02 17.78 19.05 |
0.40
0.70 1.00 1.90 |
●
● ● ● |
●
● ● ● |
Half couplings
Example of code used when ordering:
FTHCO-316L-1/4-3000
● = stock standard
Nominal pipe size | L | D | B |
Weight
|
ASTM
|
ASTM
|
---|---|---|---|---|---|---|
in. | mm | mm | mm | ~kg/pce | 304L | 316L |
1/4 3/8 1/2 3/4 |
17.4
19.1 23.8 25.4 |
19.1
22.2 28.6 34.9 |
8.13
9.14 10.92 12.70 |
0.03
0.05 0.07 0.10 |
●
● ● ● |
●
● ● ● |
1 1 ¼ 1 ½ 2 |
30.2
33.3 39.7 42.9 |
44.5
57.2 63.5 76.2 |
14.73
17.02 17.78 19.05 |
0.20
0.32 0.50 0.95 |
●
● ● ● |
●
● ● ● |
Reducing couplings
Example of code used when ordering:
FTRCO-316L-1/2-1/4-3000
● = stock standard
Nominal pipe size | L | D |
Weight
|
ASTM
|
---|---|---|---|---|
in. | mm | mm | ~kg/pce | 316L |
1/2 x 1/4 3/4 x 1/2 1 x 1/2 1 x 3/4 |
47.6
50.8 60.3 60.3 |
28.6
34.9 44.5 44.5 |
0.14
0.20 0.40 0.40 |
●
● ● ● |
1 1/4 x 1 1 1/2 x 1 1 1/2 x 1 ¼ 2 x 1 ½ |
66.7
79.4 79.4 85.7 |
57.2
63.5 63.5 76.2 |
0.70
1.00 1.10 1.90 |
●
● ● ● |