Elbows, NPT-threaded
ASTM A182 3000 lbs, ASME B16.11 / BS 3799
Elbow, 90º
Product code example:
FTE-316L-1-3000
● = stock standard
Nominal pipe size | A | D | G |
Weight
|
ASTM
|
ASTM
|
---|---|---|---|---|---|---|
in. | mm | mm | mm | ~kg/pce | 304/304L | 316/316L |
1/4 3/8 1/2 3/4 |
25
28 33 38 |
25.4
33.3 38.1 46.0 |
3.30
3.51 4.09 4.27 |
0.14
0.27 0.40 0.63 |
●
● ● ● |
●
● ● ● |
1 1 ¼ 1 ½ 2 |
44
51 60 64 |
55.6
61.9 75.4 84.1 |
4.98
5.28 5.54 7.14 |
1.10
1.22 2.35 3.30 |
●
● ● ● |
●
● ● ● |
Elbow, 45º
Example of code used when ordering:
FTE45-316L-1-3000
● = stock standard
Nominal pipe size | A | D | G |
Weight
|
ASTM
|
---|---|---|---|---|---|
in. | mm | mm | mm | ~kg/pce | 316/316L |
1/4 3/8 1/2 3/4 |
19.1
22.2 25.4 28.4 |
25.4
33.3 38.1 46.0 |
3.30
3.51 4.09 4.27 |
0.14
0.25 0.32 0.51 |
●
● ● ● |
1 1 ¼ 1 ½ 2 |
33.3
34.9 42.9 43.7 |
55.6
61.9 75.4 84.1 |
4.98
5.28 5.54 7.14 |
0.85
1.00 1.85 3.00 |
●
● ● ● |