Nipples, NPT-threaded

Tube, pipe, fittings and flanges

ASTM A182 3000 lbs, ASME B16.11 / BS 3799

Product code example:

FTHN-316L-3/8-3000

● = stock standard

3702-[Converted].png
Nominal pipe size L N
Weight
ASTM
in. mm (min.) mm ~kg/pce 316/316L
1/4
3/8
1/2
3/4
36
36
47
48
17
19
24
30
0.03
0.06
0.09
0.12



1
1 ¼
1 ½
2
59
60
62
68
35
46
50
65
0.17
0.29
0.34
0.55



-