Tees, NPT- threaded

ASTM A182 3000 lbs, ASME B16.11 / BS 3799
Product code example:
FTT-316L-2-3000
● = stock standard
Nominal pipe size | A | D | G |
Weight
|
ASTM
|
ASTM
|
---|---|---|---|---|---|---|
in. | mm | mm | mm | ~kg/pce | 304/304L | 316/316L |
1/4 3/8 1/2 3/4 |
24.6
28.6 33.3 38.1 |
25.4
33.3 38.1 46.0 |
8.13
9.14 10.92 12.27 |
0.19
0.39 0.52 0.83 |
●
● ● ● |
●
● ● ● |
1 1 ¼ 1 ½ 2 |
44.5
50.8 60.3 63.5 |
55.6
61.9 75.4 84.1 |
14.73
17.02 17.78 19.05 |
1.38
1.66 3.12 4.00 |
●
● ● ● |
●
● ● ● |