Unions, NPT-threaded

ASTM A182 3000 lbs, ASME B16.11 / BS 3799, MSS SP-83
Product code example:
FTU-316L-1-3000
● = stock standard
Nominal pipe size | L | A |
Weight
|
ASTM
|
ASTM
|
---|---|---|---|---|---|
in. | mm (min.) | mm | ~kg/pce | 304/304L | 316/316L |
1/4 3/8 1/2 3/4 |
41.4
46.0 49.0 56.9 |
19.0
22.9 27.7 33.5 |
0.13
0.20 0.40 0.50 |
●
● ● ● |
●
● ● ● |
1 1 ¼ 1 ½ 2 |
62.0
71.1 76.4 86.1 |
44.4
50.5 57.2 70.1 |
1.00
1.45 1.60 2.50 |
●
● ● ● |
●
● ● ● |