Tubes en sizes according to ISO/EN

Seamless, stainless steel tubes in sizes according to ISO/EN. For sizes below 13.5 mm (0.53 in.), see our hydraulic and instrumentation tubing program, which also includes a wide range of sizes in duplex and super-duplex stainless steels.

Need to know more?

Call us Email us

Available online

This product can be ordered online via our self-service platform E-Track, where you can also see stocks, get prices and view your order history.

E-Track is currently available in selected European countries but we are working on expanding the availability.


VIEW IN WEBSHOP


List of materials
Sandvik grade UNS ASTM EN steel no.
Sandvik 3R60™ S31603 / S31600 316L / 316 1.4435 / 1.4436
OD*,
mm
WT*,
mm
ID*, mm (nominal) ISO
thread
Kg/m Sandvik
3R60™
■ = stock standard item
13.5 2.35
8.8
1/4 in.
0.66
17.2 2.35
12.5
3/8 in.
0.87
21.3 1.6
18.1
1/2 in.
0.79
21.3 2.65
16.0
1/2 in.
1.24
26.9 1.6
23.7
3/4 in.
1.01
26.9 2.0 22.9 3/4 in. 1.24 -
26.9 2.65
21.6
3/4 in.
1.61
26.9 3.2
20.5
3/4 in.
1.90
-
30.0 2.0
26.0
1.40
33.7 2.0
29.7
1.59
33.7 2.6
28.5
2.03
-
33.7 3.25
27.2
2.48
33.7 4.05 25.6 3.01 -
38.0 2.6
32.8
2.31
42.4 2.0
38.4
1¼ in.
2.01
-
42.4 3.25
35.9
1¼ in.
3.19
44.5 2.0
40.5
2.13
44.5 2.9
38.7
3.02
48.3 2.0
44.3
1½ in.
2.32
48.3 2.6
43.1
1½ in.
2.98
48.3 3.25
41.8
1½ in.
3.67
50.0
5.0
40.0
5.61
-
51.0
2.6
45.8
3.15
54.0
2.0
50.0
2.60
57.0
2.9
51.2
3.93
60.3
2.0
56.3
2 in.
2.92
60.3
2.6
55.1
2 in.
3.76
60.3
2.9
54.5
2 in.
4.17
-
60.3
3.65
53.0
2 in.
5.18
63.5
2.6
58.3
3.97
70.0
2.9
64.2
4.87
76.1
2.0
72.1
3.71
76.1
2.9
70.3
5.32
88.9
3.6
81.7
3 in.
7.69
88.9
4.05
80.8
3 in.
8.61
101.6
3.6
94.4
8.83
108.0
4.0
100.0
10.42
114.3
3.6
107.1
4 in.
9.95
-
114.3
4.5
105.3
4 in.
12.37
121.0
4.0
113.0
11.72
133.0
4.0
125.0
12.92
159.0
4.5
150.0
17.41

* OD = outside diameter, WT = wall thickness, ID = inside diameter

Tolerances

Tolerances according to EN ISO 1127
Condition Outside diameter Wall thickness
Cold-worked +/-0.75%, but min.
+/- 0.3 mm (D3)
+/-10%, but min.
+/- 0.2 mm (T3)
Hot-worked +/-1%, but min.
+/- 0.5 mm (D2)
+/-12.5%, but min.
+/- 0.4 mm (T2)1)

1) Valid for wall thicknesses min. 4 mm and where the ratio between wall thickness and outside diameter is min. 1:10. The tolerance for other sizes is +/- 15%, but min. +/- 0.6 mm (T1).

Product standards

Sandvik 3R60™
  • PED 97/23/EC, EN 10216-5 TC1