Sandvik’s welding consumables business has been acquired by ESAB from February 1, 2018. Over the coming months ESAB will be integrating the Sandvik portfolio, to provide a smooth transition for customers. During the integration period, the full line of Sandvik welding products will continue to be accessible on this website, or via the ESAB website.

ESAB Website

Please note that the Werkstoff Nr. corresponds to the base material of the same grade.

SandvikAWS A5.11ISO 14172W.Nr.
Sanicro 53 ENiCrCoMo-1 ENi6117 2.4663
Sanicro 54 ENiCrMo-10 ENi6022 2.4602
Sanicro 56 ENiCrMo-4 ENi6276 2.4819
Sanicro 59 ENiCrMo-13 ENi6059 2.4605
Sanicro 60 ENiCrMo-3 ENi6625 2.4856
Sanicro 69 ENiCrFe-7 ENi6152 2.4627
Sanicro 71 ENiCrFe-3 ENi6182 2.4807
AquaSan Ni50 A5.35 (pending initial publication) - -