Our FCAW wire electrodes
Sandvik’s welding consumables acquired by ESAB
Sandvik’s welding consumables business has been acquired by ESAB from February 1, 2018. Over the coming months ESAB will be integrating the Sandvik portfolio, to provide a smooth transition for customers. During the integration period, the full line of Sandvik welding products will continue to be accessible on this website, or via the ESAB website.
Flux cored welding electrodes in a variety of grades and sizes for flat, horizontal or all-position welding.
Please note that the Werkstoff Nr. corresponds to the base material of the same grade.
Sandvik grade | AWS A5.22 | ISO 17633 | W.Nr. |
---|---|---|---|
19.9.L T0 | E308LT0-1/T0-4 | T 19 9 L R C 3/T 19 9 L R M 3 | 1.4316 |
19.9.L T1 | E308LT1-1/T1-4 | T 19 9 L P M 1 | 1.4316 |
19.9.H T1 | E308HT1-1/T1-4 | - | 1.4316 |
19.9.Nb T1 | E347T1-1/T1-4 | - | 1.4551 |
19.12.3.L T0 | E316T0-1/T0-4 | T 19 12 3 L R C 3/T 19 12 3 L R M 3 | 1.4430 |
19.12.3.L T1 | E316T1-1/T1-4 | T 19 12 3 L P M 2 | 1.4430 |
19.13.4.L T0 | E317T0-1/T0-4 | - | 1.4438 |
19.13.4.L T1 | E317T1-1/T1-4 | - | 1.4438 |
22.9.3.L T1 | E2209T1-1/T1-4 | T 22 9 3 N L P C M 2 | 1.4462 |
23.12.2.L T0 | E309LMoT0-1/T0-4 | T 23 12 2 L R C M 3 | 1.4333 |
23.12.2.L T1 | E309LMoT1-1/T1-4 | T 23 12 2 L R C M 1 | 1.4333 |
24.13.L T0 | E309LT0-1/T0-4 | T 23 12 L R C 3/T 23 12 L R M 3 | 1.4332 |
24.13.L T1 | E309LT1-1/T1-4 | T 23 12 L R C 2/T 23 12 L P M 2 | 1.4332 |
25.10.4.L T1 | E2594T1-1/T1-4 | - | 1.4410 |
29.9. T1 | E312T1-1/T1-4 | - | 1.4337 |