Exera™ Medical wire materials

Our EXERA™ medical wire offering includes an extensive range of stainless steels, precious metals and other biocompatible alloys, such as cobalt-chromium (CoCr) alloys.
Need to know more?
Medical wire materials (other grades can be offered on request)
Sandvik grade | UNS | ASTM |
---|---|---|
Sandvik 12R10 medical wire | S30200 | F899 |
Sandvik 11R51/11R51 HV/SH medical wire | - | 302 Mod. |
Sandvik 12R10 HV medical wire | S30400 | '304V'* |
Sandvik 5R10/2R25 medical wire | S30400/S30403 | 304/304L |
Sandvik 5R62/3R65 medical wire | S31600/S31603 | 316/316L |
Sandvik 316LVM medical wire | S31673 | F138 |
Sandvik High-N medical wire | S31675 | F1586 |
Sandvik SAF 2205 SH medical wire | S32205/S31803 | - |
Sandvik SAF 2205 medical wire | S32205/S31803 | - |
Sandvik 4C27A medical wire | S42000 | 420F* |
Sandvik 7C27 medical wire | S42000 | 420* |
Sandvik 1RK91 medical wire | S46910 | - * |
* The grade meets ASTM F899.
Sandvik grade | UNS | ASTM |
---|---|---|
Sandvik 20AP medical wire | - | - |
Sandvik Finemac | - | - |
Type of alloy | UNS | ASTM |
---|---|---|
Platinum | P04001 | B561 |
Platinum Iridium | P04010 | B684 |
Platinum Tungsten | - | - |
Platinum Clad Tantalum | - | - |
Pure Gold | P00001 | F72 |
Gold-plated Copper | - | B488 |
Silver | P07001 | B413 |
Sandvik grade | UNS | ASTM |
---|---|---|
Sandvik F562 medical wire | R30035 | F562 |
Sandvik F562 LTi medical wire* | R30035 | F562 |
* Low titanium version of Sandvik F562
Constantan |
Copper |
Kanthal Resistance Alloys
Nikrothal 80 | ||
Nikrothal 60 | ||
Nikrothal 40 | ||
Nikrothal LX | ||
Kanthal A-1 | ||
Kanthal AE | ||
Kanthal AF | ||
Kanthal D | ||
Alkrothal | ||
Cuprothal 49 | ||
Cuprothal 30 | ||
Cuprothal 15 | ||
Cuprothal 10 | ||
Cuprothal 5 | ||
Nifethal 70 | ||
Nifethal 36 |