Size range
Round wire sizes range from 0.010 to 10 mm (0.00039 to 0.394 in.), for most alloys. Other sizes available upon request.
Ribbon wire thickness ranges from 0.013 to 0.75 mm (0.0005 to 0.03 in) with aspect ratios up to 10:1. Larger aspect ratios up to 40:1 may also be available upon request.
Delivery forms
Sandvik's medical wire can be delivered in different forms, depending on size, material and end application. Some common delivery forms are:
- Spools
- Coils
- Braider bobbins
- Straightened lengths