Technical data for Wraptor ductility testing unit

Sandvik wire products acquired by Zapp AG

Sandvik’s wire business has been acquired by Zapp AG from August 31, 2018. Over the coming months Zapp will be integrating the Sandvik portfolio, to provide a smooth transition for customers. During the integration period, the full line of Sandvik wire products will continue to be accessible on this website, or via the Zapp website.

Please note: divestment of wire products does not include EXERA fine wire and medical wire components manufactured by Sandvik Palm Coast.

ZAPP WEBSITE

Sandvik's Wraptor ductility testing unit will enable a more accurate prediction of the retirement point of a slickline. This can lead to considerable cost savings through the reduced risk of unplanned production stops and the loss of valuable production equipment.

Need to know more?

Call us Email us

Construction

The ductility testing unit, Wraptor, is a sturdy construction manufactured in aluminium and stainless steel, with a 3 mm thick, high-impact resistance polymer hinged cover.

Dimensions (approx.)

Length: 18 in. (460 mm)
Width: 6 in. (150 mm)
Height: 4 in. (117 mm)

Weight

15 lbs (7 kg)

Gears

Two gear ratios are included: 1:1 and 1:2.5

Dimensional range

The dimensional range in which Wraptor will function properly is 0.072-0.160 in. (1.82-4.06 mm).

Recommended conditions for use

Recommended temperature limits are -4ºF to +122ºF (-20ºC to +50ºC). The Wraptor unit will withstand the detrimental effect of offshore sea-water environments. The gearbox is maintenance-free and will keep sand and water out.

Items included

1. Wrap test chuck
2. Wrap test bushing
3. Wire guide (plus spares)
4. Flat-nose pliers
5. Torsion test accessories
6. Allen (hex) key
7. Table fixtures
8. Handle
9. Magnifying glass (not shown in picture)
10. Wrap-test evaluation guide (not shown in picture)