Aluminium sulphate

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Ammonium bromide

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Ammonium chloride + sodium phosphate

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Ammonium hydroxide

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Ammonium perchlorate

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Ammonium sulphide

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Antimony chloride

These corrosion data are mainly based on results of general corrosion laboratory tests , carried out with pure chemicals and water solutions nearly saturated with air (the corrosion rate can be quite different if the solution is free from oxygen). All concentrations are given in weight-% and

Go to page: Previous , 1 , , 62 , 63 , 64 , 65 , 66 , 67 , 68(This page)