Swedish standard – RN78
The internal pressures are calculated by using the following formula: Where:
Attention: The pressures on these pages are given only as guidance. Dimensioning of piping systems also depends on other factors like external forces, thermal stresses, dead weight etc. Furthermore the design must be made according to regulations from local authorities and approved accordingly. For tubes in pressure vessels and boilers it is important to consider standards like TKN (Tryckkärlsnormer) 1987 and PSN (Pannsvetsnormer).
|
Sandvik | SS | 20°C | 100°C | 150°C | 200°C | 250°C | 300°C | 350°C | 400°C |
---|---|---|---|---|---|---|---|---|---|
3R12*1) | 2352 | 190 | 149 | 134 | 125 | 118 | 112 | 107 | 103 |
3R60™*2) | 2353 | 210 | 167 | 152 | 141 | 132 | 126 | 122 | 118 |
3R65*3) | 2348 | 210 | 167 | 152 | 141 | 132 | 126 | 122 | 118 |
6R35*4) | 2337 | 210 | 174 | 160 | 150 | 143 | 137 | 133 | 129 |
8R40*5) | 2338 | 220 | 181 | 167 | 158 | 150 | 145 | 140 | 136 |
5R75*6) | 2350 | 220 | 187 | 176 | 168 | 161 | 156 | 152 | 148 |
2RK65™*7) | 2562 | 220 | 175 | 165 | 155 | 145 | 135 | 130 | 125 |
Sanicro® 28*8) | 2584 | 220 | 175 | 165 | 155 | 145 | 135 | 130 | 125 |
3RE60™*9) | 2376 | 450 | 370 | 345 | 330 | 325 | 320 | ||
SAF 2304®*10) | 2327 | 400 | 315 | 290 | 275 | 265 | 255 | ||
SAF 2205™*11) | 2377 | 450 | 360 | 335 | 310 | 295 | |||
SAF 2507®*12) | 2328 | 550 | 480 | 445 | 420 | 405 |
(1 MPa = 10 bar)
*1) RN 78. t<=10mm
*2) RN 78. t<=10mm
*3) RN 78. t<=10mm
*4) RN 78. t<=10mm
*5) RN 78. t<=10mm
*6) RN 78. t<=10mm
*7) RN 78. t<=20mm
*8) NGS 1608, March 1990. OD <= 260mm, t<=10mm.
*9) NGS 1604, Sept.1983. t<= 8mm. Tmax 300°C
*10) NGS 1607, March 1992. OD <= 260mm, t<=20mm. Tmax 300°C
*11) NSG 1606, Nov 1998. OD <= 260mm, t<=24mm. Tmax 280°C. Rp0.2 is 290 MPa at 280°C, for not welded constructions
*12) NGS 1609, March 1998. OD <= 273mm, t<=20mm. Tmax 250°C