Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Pressurfect® XP is a duplex (austenitic-ferritic) stainless steel used for high pressure gasoline direct injection (GDI) fuel systems. The grade is characterized by:

  • Very good resistance to stress corrosion cracking (SCC)
  • Good resistance to general corrosion and pitting
  • High strength - approximately twice the proof strength of austenitic stainless steels
  • Physical properties that offer design advantages
  • Ease of fabrication and good toughness

Standards

  • UNS: S32304
  • EN Number: 1.4362
  • EN Name: X2CrNiN23-4

Product standards

  • ASTM A789, A790
  • EN 10216-5

Approvals

  • Approved by the American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code, Section VIII, div. 1 construction
  • ASME B31.3 Process Piping
  • VdTÜV-Werkstoffblatt 496

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.