Pressurfect®

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Pressurfect® is an austenitic stainless chromium-nickel steel with a low carbon content used for high pressure gasoline direct injection (GDI) fuel systems. The grade is characterized by:

  • Good corrosion resistance
  • Excellent toughness
  • Excellent bendability

Standards

  • ASTM: TP304L
  • UNS: S30403
  • EN Number: 1.4306
  • BS: 304S11
  • JIS: SUS304L, SUS304LTB

Product standards

  • ASTM A213, A269
  • ISO 16061
  • JIS G3459, G3463
  • EN 10216-5

Approvals

  • JIS approval for Stainless Steel Tubes
  • ASME SA213
  • ASME SA269

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.